Etching of Platinum
Etching of Platinum can be done either by wet etch or by sputtering with ions.
Comparison of Platinum Etch Methods
| Pt wet etch | IBE (Ionfab300+) | |
|---|---|---|
| Generel description | Wet etch of Pt | Sputtering of Pt |
| Etch rate range |
|
|
| Etch profile |
|
|
| Masking material |
|
|
| Substrate size |
|
Smaller pieces glued to carrier wafer
|
| Allowed materials |
No restrictions cross contamination wise as long as you use the right beaker and make sure that they are safe to enter in the chemicals |
|