'''NB: Great care has to be taken in this process due to risk of "shock-boiling" '''
'''NB: Great care has to be taken in this process due to risk of "shock-boiling" Therefore it is essential, that you stir thorough during heat up, before you start heating, at 50°C and last time at 100°C'''