Jump to content

Specific Process Knowledge/Thermal Process/BCB Curing Oven: Difference between revisions

Jehan (talk | contribs)
No edit summary
Jehan (talk | contribs)
Line 25: Line 25:
* Long curing at 250°C: BCB250AL.PDF/[[file:BCB250BL.PDF|BCB250BL.PDF]]
* Long curing at 250°C: BCB250AL.PDF/[[file:BCB250BL.PDF|BCB250BL.PDF]]


Content of BCB250BL.PDF:
Content of BCB250BL.PDF: (the file BCB210BL.PDF is identical except that the max temperature is 210 instead of 250°C)
<pre>
<pre>
;
;