'''Process recipes'''
'''Process recipes'''
*DP 2x60s: Double puddle, 2 times 60s. Rinse and dry.
*MP 4x60s: Multiple puddle, 4 times 60s. Rinse and dry.
*SP 120s: Single puddle, 120s. Rinse and dry.
*SP 120s: Single puddle, 120s. Rinse and dry.
*SP 15s: Single puddle, 15s. Rinse and dry.
*SP 30s: Single puddle, 30s. Rinse and dry.
*SP 30s: Single puddle, 30s. Rinse and dry.
*SP 60s: Single puddle, 60s. Rinse and dry.
*SP 60s: Single puddle, 60s. Rinse and dry.