LabAdviser/Technology Research/Fabrication of Hyperbolic Metamaterials using Atomic Layer Deposition/EMT Procces flow: Difference between revisions
Appearance
| Line 57: | Line 57: | ||
!2.4 | !2.4 | ||
|TiO<sub>2</sub>/Al<sub>3</sub>O<sub>3</sub> multilayers deposition using Atomic Layer Deposition | |TiO<sub>2</sub>/Al<sub>3</sub>O<sub>3</sub> multilayers deposition using Atomic Layer Deposition | ||
|Deposition using recipies EMA01, EMA02, EMA03 and EMA04. | |Deposition using recipies <b>EMA01</b>, <b>EMA02</b>, <b>EMA03</b> and <b>EMA04</b>. | ||
|[[Specific_Process_Knowledge/Thin_film_deposition/ALD_Picosun_R200|ALD Picosun R200]], Recipies performance [[Specific_Process_Knowledge/Thin_film_deposition/ALD_Picosun_R200/ALD_multilayers#Low_temperature_grown_multilayers_on_flat_surfaces|Multilayrs recipies and their performance]] . | |[[Specific_Process_Knowledge/Thin_film_deposition/ALD_Picosun_R200|ALD Picosun R200]], Recipies performance [[Specific_Process_Knowledge/Thin_film_deposition/ALD_Picosun_R200/ALD_multilayers#Low_temperature_grown_multilayers_on_flat_surfaces|Multilayrs recipies and their performance]] . | ||
|[[image:2 lithography mask 1.jpg|250x350px|center]] | |[[image:2 lithography mask 1.jpg|250x350px|center]] | ||