Jump to content

Specific Process Knowledge/Thermal Process/Dope with Phosphorus: Difference between revisions

Kabi (talk | contribs)
No edit summary
Kabi (talk | contribs)
Line 200: Line 200:
|-
|-
! Aug2012  
! Aug2012  
| 48
| 47.0
| 93.1  
| 93.1  
| 41.8
| 41.8
Line 212: Line 212:
|-
|-
! Aug2013  
! Aug2013  
| 58
| 58.0
| 91,8
| 91.8
| 41,8
| 41.8
   
   
|-
|-