Jump to content

Specific Process Knowledge/Thermal Process/Furnace: Multipurpose annealing: Difference between revisions

From LabAdviser
Pevo (talk | contribs)
Pevo (talk | contribs)
Line 15: Line 15:
[[Image:ATV_ovn_boat.jpg|thumb|350x350px|Boat with wafer for the multipurpose annealing furnace.]]
[[Image:ATV_ovn_boat.jpg|thumb|350x350px|Boat with wafer for the multipurpose annealing furnace.]]


The purpose of the ATV Furnace is to...
The purpose of the ATV Furnace is annealing and oxidation of different samples and resist pyrolysis. Annealling and resist pyrolysis can be done in vaccum or at atmospheric pressure, in a N</sub>2<sub> , H</sub>2<sub> or a mixture of the two gasses.  


Is is possible to change all quartz ware in the furnace (the furnace tube and door and the wafer boat), so that different furnace tubes can he
Is is possible to change all quartz ware in the furnace (the furnace tube, the door sealing and the wafer boat). A the moment we have two different sets of quartz ware - One that is dedicated for resist pyrolysis, and one that is dedicated for annealing of oxidation of different sample, e.g. samples with metals. The quartz ware is normally changed once a week.


The furnace is heated by use on 12 long heaters that are situated along the furnace tube and two flat heaters that are situated in the ends of the furnace tube. The that way the temperature will be very uniform everywhere in the furnace tube. For atmospheric pressure processes the maximum temperature is 1100 <sup>o</sup>C, and for vacuum processes the maximum temperature is 1050 <sup>o</sup>C.
The furnace tube is heated by use on 12 long heaters that are situated along the furnace tube and two flat heaters that are situated in the ends of the furnace tube. The that way the temperature will be very uniform everywhere in the furnace tube. For atmospheric pressure processes the maximum temperature is 1100 <sup>o</sup>C, and for vacuum processes the maximum temperature is 1050 <sup>o</sup>C.
Very fast heating..
Very fast heating..



Revision as of 12:01, 5 August 2015

THIS PAGE IS UNDER CONSTRUCTION

Multipurpose annealing furnace

Feedback to this page: click here

The ATV Furnace

Multipurpose annealing furnace. Positioned in cleanroom B-1
Boat with wafer for the multipurpose annealing furnace.

The purpose of the ATV Furnace is annealing and oxidation of different samples and resist pyrolysis. Annealling and resist pyrolysis can be done in vaccum or at atmospheric pressure, in a N2 , H2 or a mixture of the two gasses.

Is is possible to change all quartz ware in the furnace (the furnace tube, the door sealing and the wafer boat). A the moment we have two different sets of quartz ware - One that is dedicated for resist pyrolysis, and one that is dedicated for annealing of oxidation of different sample, e.g. samples with metals. The quartz ware is normally changed once a week.

The furnace tube is heated by use on 12 long heaters that are situated along the furnace tube and two flat heaters that are situated in the ends of the furnace tube. The that way the temperature will be very uniform everywhere in the furnace tube. For atmospheric pressure processes the maximum temperature is 1100 oC, and for vacuum processes the maximum temperature is 1050 oC. Very fast heating..

For resist pyrolysis, where samples with different resist layers are heated up to maximum 1100 oC in a nitrogen atmosphere. At high temperatures carbon is formed by pyrolysis of the resist. In this way conductive structures can be made from a resist patterned sample. If oxygen from the air or from outgassing of the resist is present in the furnace, the resist layer will be removed, thus it is important to evacuate the furnace and flush it with nitrogen, before a high temperature for resist pyrolysis is obtained. Pyrolysis of a large amount of resist may also be a problem due to resist outgassing.

During processing the furnace is rapidly heated by use of six long heating lamps situated around the furnace tube, and cooling is done (rather slowly) by use of cooling fans. The furnace is purged with a controlable nitrogen flow. There is no vacuum on the furnace.

The ATV Furnace was installed in the cleanroom in 2014.

The user manual, technical information and contact information can be found in LabManager:

Furnace: ATV

Process information

Overview of the performance of the ATV furnace and process related parameters

Purpose
  • Dry oxidation of silicon
  • Annealing in N2 and H2
  • Pyrolysis of different resists
Performance Film thickness
  • Dry SiO2: 50 Å to ~2000 Å (it takes too long to grow a thicker oxide)
Process parameter range Process Temperature
  • No vacuum: 25 oC - 1100 oC
  • Vacuum: 25 oC - 1050 oC
Process pressure
  • 1 atm
  • Vacuum down to ~0.1 mbar
Gasses on the system
  • N2
  • O2
  • H2
Substrates Batch size
  • 1-30 50 mm, 100 mm or 150 mm wafers per run
  • 1-50 200 mm wafers per run
Substrate materials allowed
  • Depends on furnace tube