==AZ 4562==
==AZ 4562==
[[Image:RCD8 AZ 5214E.jpg|300x300px|thumb|right|Spin curve for AZ 4562]]
[[Image:RCD8 AZ 4562.jpg|300x300px|thumb|right|Spin curve for AZ 4562]]
Spin coating of AZ 5214E on Spin Coater: RCD8 using manual dispense is a very simple process. The wafer is accelerated at 1000rpm/s to the spin-off speed, spun for 30s, then decelerated at 1000rpm/s.
Spin coating of AZ 5214E on Spin Coater: RCD8 using manual dispense is a very simple process. The wafer is accelerated at 1000rpm/s to the spin-off speed, spun for 30s, then decelerated at 1000rpm/s.