'''Feedback to this section''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Lithography/Coaters#Manual_Spinner_1 click here]''' | '''Feedback to this section''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Lithography/Coaters#Manual_Spinner_1 click here]''' | ||
[[Specific_Process_Knowledge/Lithography/Coaters#Coaters:_Comparison_Table|Coater comparison table]] | |||
Manual Spinner 1, WS-650 model, from Laurell is a resist spinning coater at Danchip which can be used for spinning on whole 2", 4" and 6" substrates and also a small pieces. | Manual Spinner 1, WS-650 model, from Laurell is a resist spinning coater at Danchip which can be used for spinning on whole 2", 4" and 6" substrates and also a small pieces. | ||