Jump to content

Specific Process Knowledge/Etch/DRIE-Pegasus/showerheadchange/polySi/Cpoly2: Difference between revisions

From LabAdviser
Jmli (talk | contribs)
Created page with " {| border="2" cellpadding="0" cellspacing="0" style="text-align:center;" |+ '''Process runs''' |- ! rowspan="2" width="40"| Date ! colspan="4" width="120"| Substrate Informat..."
 
Jmli (talk | contribs)
No edit summary
Line 23: Line 23:
| Pegasus/jmli
| Pegasus/jmli
| 10 minute TDESC clean + 45 sec barc etch
| 10 minute TDESC clean + 45 sec barc etch
| danchip/showerhead/polySi etch DUV mask, 20 cycles or 2:08 minutes  
| danchip/jml/showerhead/Cpoly2, 20 cycles or 2:08 minutes  
| S004729
| S004729
| New showerhead  
| New showerhead  

Revision as of 14:54, 11 December 2014

Process runs
Date Substrate Information Process Information SEM Images
Wafer info Mask Material/ Exposed area Tool / Operator Conditioning Recipe Wafer ID Comments
3/12-2014 1/4 6" Wafer with 210 nm oxide and 1800 nm polysilicon CB on oxide carrier standard stepper mask (50 nm barc + 320 nm krf) Si / 50+ % Pegasus/jmli 10 minute TDESC clean + 45 sec barc etch danchip/jml/showerhead/Cpoly2, 20 cycles or 2:08 minutes S004729 New showerhead

File:S004729-01.jpg File:S004729-02.jpg File:S004729-03.jpg