Jump to content

Specific Process Knowledge/Back-end processing/Laser Micromachining Tool/fluence: Difference between revisions

From LabAdviser
Chasil (talk | contribs)
Chasil (talk | contribs)
Line 23: Line 23:
![[image:140414_FluenceVSrepRate_1064nm_255mm_v3.jpg|500x500px|thumb|center|Fluence result for IR wavelength (1064nm, F255mm)]]
![[image:140414_FluenceVSrepRate_1064nm_255mm_v3.jpg|500x500px|thumb|center|Fluence result for IR wavelength (1064nm, F255mm)]]
![[image:140414_FluenceVSrepRate_532nm_255mm_v3.jpg|500x500px|thumb|center|Fluence result for green wavelength (532nm, F255mm)]]
![[image:140414_FluenceVSrepRate_532nm_255mm_v3.jpg|500x500px|thumb|center|Fluence result for green wavelength (532nm, F255mm)]]
![[image:140526_FluenceVSrepRate_355nm_100mm.jpg|500x500px|thumb|center|Fluence result for UV wavelength (355nm, F100mm)]]
![[image:140526_FluenceVSrepRate_355nm_255mm.jpg.jpg|500x500px|thumb|center|Fluence result for UV wavelength (355nm, F100mm)]]
|}
|}
{| border="1" cellspacing="2" cellpadding="2"  
{| border="1" cellspacing="2" cellpadding="2"  

Revision as of 09:15, 4 August 2014

Fluence definition

The fluence produces by a laser is, by definition, the energy delivered by a laser pulse (Epulse) per surface unit (A) and it is given in J/cm2.


The function Epulse is defined as :


Epulse=P‾f

Where P‾ (average power) is measured with the laser sensor power measurement (see manual,section 5.3) and the repetion rate (f) is set in the parameter file under " laser frequency".

The fluence is therefore determinated as such :


Fluence=EpulseA

The area (A) can be determinate with the theoretical min spot diameter (1/e2), available here

Fluence results measurement

Fluence result for IR wavelength (1064nm, F255mm)
Fluence result for green wavelength (532nm, F255mm)
File:140526 FluenceVSrepRate 355nm 255mm.jpg.jpg
Fluence result for UV wavelength (355nm, F100mm)
Fluence result for IR wavelength (IPG 1064nm, F255mm)