'''AZ 5214E and AZ 4562''' | '''AZ 5214E and AZ 4562''' | ||
*1.5µm: 35-49 mJ/cm<sup>2<sup> corresponding to 5-7 seconds exposure at 7 mW/ | Compared to exposure on Aligner-6inch, the dose on KS-Aligner is doubled. | ||
*1.5µm: 35-49 mJ/cm<sup>2</sup> corresponding to 5-7 seconds exposure at 7 mW/cm<sup>2</sup>. | |||