====Procedure for making a new developer==== | ====Procedure for making a new developer==== | ||
1. 800ml "Developer AZ | 1. 800ml "Developer AZ 351B" is mixed with 4000ml water in a special container in the fume hood. | ||
2. Fill the bath with the developer mixture and heat it to 22 °C before use. | 2. Fill the bath with the developer mixture and heat it to 22 °C before use. | ||