= DUV Stepper FPA-3000EX4 from Canon =
= DUV Stepper=


[[Image:stepper_image_1.jpg|200×200px|right|thumb|DUV Stepper is placed in F-3]]
[[Image:stepper_image_1.jpg|200×200px|right|thumb|DUV Stepper is placed in F-3]]
Line 5: Line 5:
'''Feedback to this section''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php?title=Specific_Process_Knowledge/Lithography/DUVStepperLithography#DUV_Stepper_FPA-3000EX4_from_Canon click here]'''
'''Feedback to this section''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php?title=Specific_Process_Knowledge/Lithography/DUVStepperLithography#DUV_Stepper_FPA-3000EX4_from_Canon click here]'''


The FPA-3000EX4 is an advanced exposure system designed for mass-production of 6 and 8 inch large wafers/ devices. The largest applicable thickness of the wafers/ devices is 1,2 mm. Also 4" wafers/ devices can be processed with some restrictions concerning throughput, resolution, uniformity and maximum allowed wafer thickness. The system is equipped with a KrF Excimer laser from Cymer (wavelength 248 nm) leading to a specified resolution of 250 nm that is improved when well-defined pattern designs are used. The best resolution could be achieved with single line structures (line widths down to 160 nm) and multi-line structures (line widths down to 180 nm).
The FPA-3000EX4 from Canon is an advanced exposure system designed for mass-production of 6 and 8 inch large wafers/ devices. The largest applicable thickness of the wafers/ devices is 1,2 mm. Also 4" wafers/ devices can be processed with some restrictions concerning throughput, resolution, uniformity and maximum allowed wafer thickness. The system is equipped with a KrF Excimer laser from Cymer (wavelength 248 nm) leading to a specified resolution of 250 nm that is improved when well-defined pattern designs are used. The best resolution could be achieved with single line structures (line widths down to 160 nm) and multi-line structures (line widths down to 180 nm).