Jump to content

Specific Process Knowledge/Thermal Process/Jipelec RTP: Difference between revisions

From LabAdviser
Mdyma (talk | contribs)
Bghe (talk | contribs)
No edit summary
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:thinfilm@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thermal_Process/Jipelec_RTP click here]'''
'''Feedback to this page''': '''[mailto:thinfilm@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thermal_Process/Jipelec_RTP click here]'''
[[Category: Equipment |Furnace]]
[[Category: Thermal process|Furnace]]
[[Category: Furnaces|Jipelec]]


==Jipelec - Rapid Thermal Processing==
==Jipelec - Rapid Thermal Processing==

Revision as of 14:35, 25 August 2014

Feedback to this page: click here

Jipelec - Rapid Thermal Processing

Jipelec RTP: Positioned in cleanroom A-4

The Jipelec is a rapid thermal processing (RTP) oven. It is be used for fast and well-controlled annealing or alloying of samples. It is possible to use either a thermocouple or a pyrometer to control the temperature (of the sample carrier).


The user manual, technical information and contact information can be found in LabManager:

Jipelec RTP

Overview of the performance of the Jipelec RTP and some process related parameters

Purpose RTP annealing
Process parameter range Process Temperature
  • 0-1000 oC
  • Temperature ramp up to 300 oC/min
Process pressure
  • 1 atm
  • Vacuum
Gasses on the system
  • N2
Substrates Batch size
  • One 100 mm wafer (or 50 wafer) per run
  • Small samples (placed on a carbide carrier or a Si carrier wafer with 1 µm oxide)
Substrate material allowed

A silicon carrier wafer with 1 µm oxide is always need (except for III-V materials)

  • Silicon
  • Silicon oxides
  • Silicon nitrides
  • Quartz
  • Polysilicon
  • Titan
  • III-V materials (on graphite carrier)
  • Silicon wafers (new from the box or RCA cleaned)
  • In doubt: look at the cross contamination chart or send a mail to the Furnace group.