Specific Process Knowledge/Etch/Wet Titanium Etch: Difference between revisions
Appearance
No edit summary |
|||
| Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:wetchemistry@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Wet_Titanium_Etch click here]''' | '''Feedback to this page''': '''[mailto:wetchemistry@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Wet_Titanium_Etch click here]''' | ||
[[Category: Equipment|Etch Wet Titanium]] | |||
[[Category: Etch (Wet) bath|Titanium]] | |||
Ething of Titanium can be done either wet or dry. For wet etching please see below on this page. Dry etching can be done either with [[Specific Process Knowledge/Etch/ICP Metal Etcher|ICP]] using Chlorine chemistry or with [[Specific Process Knowledge/Etch/IBE/IBSD Ionfab 300|IBE]] by sputtering with Ar ions. | Ething of Titanium can be done either wet or dry. For wet etching please see below on this page. Dry etching can be done either with [[Specific Process Knowledge/Etch/ICP Metal Etcher|ICP]] using Chlorine chemistry or with [[Specific Process Knowledge/Etch/IBE/IBSD Ionfab 300|IBE]] by sputtering with Ar ions. | ||