Jump to content

Specific Process Knowledge/Back-end processing/Laser Micromachining Tool: Difference between revisions

Chasil (talk | contribs)
Chasil (talk | contribs)
Line 144: Line 144:
| 50 µm
| 50 µm
| [[media:Dicing_Si_Si3N4_1064nm_f255mm.xls|Silicon nitride cutting parameters]]
| [[media:Dicing_Si_Si3N4_1064nm_f255mm.xls|Silicon nitride cutting parameters]]
| Samples can easily be removed with a soft mecanical pressure. A layer of resist can be deposited on the top without influence the dicing.  
| Samples can easily be removed with a soft mechanical pressure. A layer of resist can be deposited on the top without influenced the dicing.
|-
|-
|- style="background:LightGray;text-align:center" valign="top"
|- style="background:LightGray;text-align:center" valign="top"