Jump to content

Specific Process Knowledge/Lithography/LiftOff: Difference between revisions

From LabAdviser
Tigre (talk | contribs)
Created page with "==Lift-off wet bench== 300x300px|thumb|Acetone lift-off: positioned in cleanroom 3 This bench is only for wafers with metal! Here are the main ..."
 
Tigre (talk | contribs)
Line 1: Line 1:
==Lift-off wet bench==
=Lift-off Wet Bench=
[[Image:Acetone_lift-off.jpg|300x300px|thumb|Acetone lift-off: positioned in cleanroom 3]]
[[Image:Acetone_lift-off.jpg|300x300px|thumb|Acetone lift-off: positioned in cleanroom 3]]
This bench is only for wafers with metal!
This bench is only for wafers with metal!

Revision as of 13:38, 9 August 2013

Lift-off Wet Bench

Acetone lift-off: positioned in cleanroom 3

This bench is only for wafers with metal!

Here are the main rules for lift-off bench use:

  • Place the wafers in a dedicated wafer holder.
  • Put the holder in the acetone and start the ultrasound. The strip off time is depending of resist thickness.
  • Rinse your wafers for 4-5 min. in running water after stripping.

Find more info about the lift-off process here: Specific Process Knowledge/Photolithography/AZ5214E standard resist - reverse process