Specific Process Knowledge/Thin film deposition/Deposition of Silicon Oxide/Deposition of Silicon Oxide using PECVD: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 39: | Line 39: | ||
===Expected results=== | ===Expected results=== | ||
{| border="1" cellspacing="0" cellpadding=" | {| border="1" cellspacing="0" cellpadding="6" | ||
|- | |- | ||
|Recipe name | |Recipe name | ||