Jump to content

Specific Process Knowledge/Thin film deposition/Deposition of Chromium/Thermal evaporation of Cr in Thermal evaporator: Difference between revisions

Eves (talk | contribs)
Eves (talk | contribs)
Line 217: Line 217:
</gallery>
</gallery>


The limited amount of chromium, the nature of deposition (in all directions) and retruction sets a limit on how thick layer can be deposited. We do not recomend to exeed the thickness above 80 nm, and do not allow thicknesses above 100 nm.


Note! <b>Remember to discard the used tungsten rods. Never reinstall them. Always mount a new source.</b>
Note! <b>Remember to discard the used tungsten rods. Never reinstall them. Always mount a new source.</b>