Specific Process Knowledge/Thin film deposition/Deposition of Chromium/Thermal evaporation of Cr in Thermal evaporator: Difference between revisions
Appearance
| Line 230: | Line 230: | ||
</gallery> | </gallery> | ||
The following model is selected for XRR fitting: Native chromium oxide, bulk chromium layer, native silicon oxide, and the bulk silicon substrate. Fitting | The following model is selected for XRR fitting: Native chromium oxide, bulk chromium layer, native silicon oxide, and the bulk silicon substrate. Fitting results presented in the table. | ||