'''*''' The deposition rate can be increased (up to 2Å/s or even 5 Å/s), but it requires a new recipe.  
'''*''' The deposition rate can be increased (up to 2Å/s or even 5 Å/s), but it requires a new recipe.  


'''**'''Although it is possible to deposit 100 nm, we do not recommend exceeding the thickness setpoint above 80 nm, due to instabilities at the end.
'''**'''Although it is possible to deposit 100 nm, we do not recommend exceeding the thickness setpoint above <b>80 nm</b>, due to instabilities at the end.