=== '''Third run''' ===
=== '''Deposition of 100 nm''' ===


The adjusted tooling factor 173% was fine. Full 6" wafer is loaded for film characterisation. Measured base pressure before start 4.4 10<sup>-6</sup> Torr. Waited 1 hour before start. Deposition thickness setpoint is set to 100 nm.
The adjusted tooling factor 173% was fine. Full 6" wafer is loaded for film characterisation. Measured base pressure before start 4.4 10<sup>-6</sup> Torr. Waited 1 hour before start. Deposition thickness setpoint is set to 100 nm.