==Spin Coater: RCD8==
==Spin Coater: RCD8==
[[Image:Spinner_RCD8_C-1.jpg|400px|thumb|Spin coater: RCD8 is located in C-1]]
[[Image:Spinner_RCD8_C-1.jpg|400px|thumb|Spin coater: RCD8 is located in E-4]]


Spin Coater: RCD8 is a model RCD8 T spin coater from Süss MicroTec with a motorized media arm and Gyrset functionality. It's primary purpose is spin coating of SU-8 resist. The media arm was disabled in 2024.
Spin Coater: RCD8 is a model RCD8 T spin coater from Süss MicroTec with a motorized media arm and Gyrset functionality. It's primary purpose is spin coating of SU-8 resist. The media arm was disabled in 2024.
Line 10: Line 10:
===[[Specific Process Knowledge/Lithography/Coaters/Spin Coater: RCD8 processing|Process information]]===
===[[Specific Process Knowledge/Lithography/Coaters/Spin Coater: RCD8 processing|Process information]]===
*[[Specific Process Knowledge/Lithography/Coaters/Spin Coater: RCD8 processing#Spin coating|Spin coating]]
*[[Specific Process Knowledge/Lithography/Coaters/Spin Coater: RCD8 processing#Spin coating|Spin coating]]
*[[Specific Process Knowledge/Lithography/Coaters/Spin Coater: RCD8 processing#Automatic dispense|Automatic dispense]]
*[[Specific Process Knowledge/Lithography/Coaters/Spin Coater: RCD8 processing#Dispense|Dispense]]
*[[Specific Process Knowledge/Lithography/Coaters/Spin Coater: RCD8 processing#Recipes|Recipes and templates]]
*[[Specific Process Knowledge/Lithography/Coaters/Spin Coater: RCD8 processing#Recipes|Recipes and templates]]
*[[Specific Process Knowledge/Lithography/Coaters/Spin Coater: RCD8 processing#Processing_results|Processing results]]
*[[Specific Process Knowledge/Lithography/Coaters/Spin Coater: RCD8 processing#Processing_results|Processing results]]
Line 24: Line 24:
*Spin coating of PGMEA based AZ resists
*Spin coating of PGMEA based AZ resists
*Spin coating of wafers with structured backside
*Spin coating of wafers with structured backside
*Edge bead removal
*(Edge bead removal)
|-
|-
!style="background:silver; color:black;" align="center" width="60"|Resist  
!style="background:silver; color:black;" align="center" width="60"|Resist  
Line 30: Line 30:
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
* manual dispense
* manual dispense
* automatic dispense from syringe
* <strike>automatic dispense from syringe</strike>
|-
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="1"|Performance
!style="background:silver; color:black" align="center" valign="center" rowspan="1"|Performance
|style="background:LightGrey; color:black"|Coating thickness
|style="background:LightGrey; color:black"|Coating thickness
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
* SU-8 resits: 0.1-200+ µm
* SU-8 resists: 0.1-200+ µm
* AZ 5214E: 1.5-3 µm
* AZ 5214E: 1.5-3 µm
* AZ 4562: 8-15 µm
* AZ 4562: 8-15 µm

Latest revision as of 09:23, 3 November 2025

Spin Coater: RCD8

Spin coater: RCD8 is located in E-4

Spin Coater: RCD8 is a model RCD8 T spin coater from Süss MicroTec with a motorized media arm and Gyrset functionality. It's primary purpose is spin coating of SU-8 resist. The media arm was disabled in 2024.

However, due to the possibility of using a non-vacuum chuck, the spin coater is also suitable for coating of substrates with e.g. textured backsides or membranes.

The user manual, user APV, and contact information can be found in LabManager - requires login

Process information

Equipment performance and process related parameters

Purpose
  • Spin coating of SU-8 resists
  • Spin coating of PGMEA based AZ resists
  • Spin coating of wafers with structured backside
  • (Edge bead removal)
Resist
  • manual dispense
  • automatic dispense from syringe
Performance Coating thickness
  • SU-8 resists: 0.1-200+ µm
  • AZ 5214E: 1.5-3 µm
  • AZ 4562: 8-15 µm
  • AZ MiR 701: 1.5-3 µm
  • AZ nLOF 2020: 2-3.5 µm
Process parameters Spin speed

Vacuum chuck: 10 - 5000 rpm
Non-vacuum chuck: Max. 3000 rpm

Spin acceleration

10 - 3000 rpm/s
Max. 1500 rpm/s with Gyrset

Substrates Substrate size
  • 100 mm wafers
  • 150 mm wafers (vacuum chuck only)
Allowed materials

All cleanroom materials ?

Batch

1