Jump to content

Specific Process Knowledge/Thin film deposition/Deposition of Silicon Oxide/Deposition of SiO2 in E-Beam Evaporator Temescal-2: Difference between revisions

Eves (talk | contribs)
Eves (talk | contribs)
No edit summary
 
(2 intermediate revisions by the same user not shown)
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Silicon_Oxide/Deposition_of_SiO2_in_E-Beam_Evaporator_Temescal-2 click here]'''
<i>This page is written by <b>Evgeniy Shkondin @DTU Nanolab</b> if nothing else is stated. <br>
<i>This page is written by <b>Evgeniy Shkondin @DTU Nanolab</b> if nothing else is stated. <br>
All images and photos on this page belongs to <b>DTU Nanolab</b>.<br>
All images and photos on this page belongs to <b>DTU Nanolab</b>.<br>
Line 91: Line 93:
=Optical functions=
=Optical functions=


Results have been obtained for <100> 150 mm Si wafers with native oxide, based on ellipsometry study. Sellmeier model has been implemented for refractive index fitting.
Results have been obtained for <100> 150 mm Si wafers with native oxide, based on [[Specific_Process_Knowledge/Characterization/Optical_characterization#Ellipsometer|ellipsometry study]]. Sellmeier model has been implemented for refractive index fitting.