Specific Process Knowledge/Etch/Aluminum Oxide/Al2O3 Etch with ICP Metal: Difference between revisions
Appearance
| Line 7: | Line 7: | ||
|-style="background:Black; color:White" | |-style="background:Black; color:White" | ||
! Parameter | ! Parameter | ||
|Recipe name: ''' | |Recipe name: '''Al2O3 Etch''' | ||
|- | |- | ||
|Coil Power [W] | |Coil Power [W] | ||