Specific Process Knowledge/Thin film deposition/Deposition of Scandium: Difference between revisions
Appearance
Created page with "'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Scandium&action=submit click here]''' <i> Unless otherwise stated, this page is written by <b>DTU Nanolab internal</b></i> == Deposition of Scandium == Deposition of Sc can only be done by sputtering using 4-inch Sc target. The only tool for this applicatio..." |
mNo edit summary |
||
| Line 1: | Line 1: | ||
{{cc-nanolab}} | |||
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Scandium&action=submit click here]''' | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Scandium&action=submit click here]''' | ||
== Deposition of Scandium == | == Deposition of Scandium == | ||
Latest revision as of 19:23, 10 June 2025
The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.
Feedback to this page: click here
Deposition of Scandium
Deposition of Sc can only be done by sputtering using 4-inch Sc target.
The only tool for this application is the Cluster-based multi-chamber high vacuum sputtering deposition system, commonly referred to as the 'Cluster Lesker.' The operating process is thoroughly documented and described in detail.:
- Deposition of Scandium (Sc) using sputtering in Sputter-System Metal-Nitride(PC3) Source 1 (4-inch target)
At the moment (October 2023) we have a 4-inch Sc target (0.250" thick bonded to Cu) for PC3 Src1.