=Micro Transfer Printer= | =Micro Transfer Printer= | ||
Micro transfer printing is an emerging technique to transfer diverse and non-native components from source substrate to target substrate. Micro transfer printing is best for achieving heterogeneous integration, | |||
where micro-components from different sources are picked up by polymer stamp and precisely assembled onto different target substrate such as glass, plastic, ceramic and silicon. This method is known for | |||
increasing functionality and improving efficiency. | |||
Micro transfer printer 1003 from Xdisplay was installed in year 2022 and placed in cleanroom F-4. | |||
Micro transfer printer | |||
Equipment info in [http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=503 Lab Manager] - '''requires login''' | Equipment info in [http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=503 Lab Manager] - '''requires login''' | ||
[[Image:Equipment.jpg|500x500px|thumb|The Micro transfer printer is placed in F-4]] | |||
[[Image:MTP image.jpg|1000px|thumb|left|Steps involved in pick and print]] | |||
<br clear="all" /> | <br clear="all" /> | ||
==Equipment performance and process related parameters== | ==Equipment performance and process related parameters== | ||
{|border="1" cellspacing="1" cellpadding="10" style="text-align:left;" | {|border="1" cellspacing="1" cellpadding="10" style="text-align:left;" | ||