Jump to content

LabAdviser/314/Microscopy 314-307/TEM/Tips/HAADF-detector: Difference between revisions

From LabAdviser
Jenk (talk | contribs)
Jenk (talk | contribs)
mNo edit summary
 
(One intermediate revision by the same user not shown)
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/LabAdviser/Microscopy_314-307/314/ATEM/HAADF-detector click here]'''
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/LabAdviser/Microscopy_314-307/314/ATEM/HAADF-detector click here]'''


(''content by Jens Kling, January 2021'')
(''content by Jens Kling @DTU Nanolab, January 2021'')
[[Category:314]]
[[Category:314]]
[[Category:314-Microscopy]]
[[Category:314-Microscopy]]


= HAADF detector doesn't give a signal =
= HAADF detector doesn't give a signal =

Latest revision as of 16:03, 9 September 2026

Feedback to this page: click here

(content by Jens Kling @DTU Nanolab, January 2021)

HAADF detector doesn't give a signal

Eventhough the HAADF detector is inserted properly, it sometimes doesn't give a signal. This is typically the case at the beginning of the session, when the detector is used for the first time. If this is the case, try the following:

  1. Go to the "STEM Detector (User)" control panel
  2. Open the flapout
  3. Un-check "HAADF"
  4. Check "HAADF"
  5. Try imaging again. The detector should give a signal.