Specific Process Knowledge/Characterization/Optical microscope: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| (32 intermediate revisions by 7 users not shown) | |||
| Line 1: | Line 1: | ||
{{cc-nanolab}} | |||
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/Optical_microscope click here]''' | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/Optical_microscope click here]''' | ||
| Line 4: | Line 6: | ||
[[Category: Characterization|Optical mi]] | [[Category: Characterization|Optical mi]] | ||
{|border="1" cellspacing="1" cellpadding="3" style="text-align:left;" | |||
|- | |||
|-style="background:white; color:black; vertical-align:middle; text-align:center;" | |||
| | |||
!Noco IR | |||
! | !Leica<br>INM 100 | ||
!Zeiss<br>Jenatech | |||
!Nikon Eclipse<br>L200 #1 | |||
! Leica | !Nikon Eclipse<br>L200 #2 | ||
!Nikon Eclipse<br>L200N #3 | |||
!Nikon Eclipse<br>L200N #4 | |||
! Zeiss Jenatech | !Nikon<br>ME 600 | ||
!Leica<br>S8 APO | |||
!Zeiss<br>Axiotron | |||
!Olympus<br>MX63 | |||
! Nikon Eclipse L200 | |||
! Nikon Eclipse L200 | |||
! Nikon | |||
! Nikon | |||
|- | |- | ||
|- | |||
|-style="background:white; color:black; vertical-align:middle; text-align:center;" | |||
| | | | ||
|[[image: | |[[image:Noco IR microscope.jpg|100x100px|thumb|center]][[image:Noco IR microscope_1.jpg|100x100px|thumb|center]] | ||
[[image: | |[[image:LeicaINM100.jpg|100x100px|thumb|center]] | ||
|[[image: | |[[image:Zeiss Jenatech strain.jpg|100x100px|thumb|center]][[image:Zeiss Jenatech strain_1.jpg|100x100px|thumb|center]] | ||
|[[image: | |[[image:Nikon Eclipse L200.jpg|100x100px|thumb|center]][[image:Nikon Eclipse L200_1.jpg|100x100px|thumb|center]] | ||
|[[image:Nikon Eclipse L200 2.jpg|100x100px|thumb|center]][[image:Nikon Eclipse L200 2_1.jpg|100x100px|thumb|center]] | |||
|[[image: | |[[image:Nikon Eclipse L 200 3_1.jpg|100x100px|thumb|center]] | ||
[[image: | |[[image:Nikon Eclipse L 200 4_1.jpg|100x100px|thumb|center]] | ||
|[[image: | |[[image:Nikon ME 600.jpg|100x100px|thumb|center]][[image:Nikon ME 600_1.jpg|100x100px|thumb|center]] | ||
[[image: | |[[image:Leica S8 APO.jpg|100x100px|thumb|center]] | ||
|[[image: | |[[image:Zeiss Axiotron.jpg|100x100px|thumb|center]][[image:Zeiss Axiotron_1.jpg|100x100px|thumb|center]] | ||
|[[File:View front right .jpg|100x100px|thumb|center]] | |||
|[[image:Nikon | |- | ||
[[image:Nikon ME 600_1.jpg|100x100px|thumb| | |- | ||
|[[image: | |-style="background:LightGrey; color:black; vertical-align:middle; text-align:left;" | ||
!Location | |||
|[[image: | |||
[[image: | |||
|[[File: | |||
|- | |||
| | |||
|- | |||
| | |346-901 | ||
| | |346-901 | ||
| | |cleanroom<br>D-3 | ||
| | |cleanroom<br>D-3 | ||
| | |cleanroom<br>A-1 | ||
| | |cleanroom<br>D-3 | ||
| | |cleanroom<br>E-5 | ||
|cleanroom<br>F-1 | |||
|cleanroom<br>Cx1 | |||
|cleanroom<br>F-3 | |||
|cleanroom<br>E-4 | |||
|- | |||
|- | |||
|-style="background:WhiteSmoke; color:black; vertical-align:middle; text-align:left;" | |||
!Responsible<br>group | |||
|Wet chemistry | |||
|Wet chemistry | |||
|Lithography | |||
|Lithography | |||
|Lithography | |||
|Lithography | |||
|Lithography | |||
|Lithography | |||
|Lithography | |||
|Lithography | |||
|Lithography | |||
|- | |||
|- | |||
|-style="background:LightGrey; color:black; vertical-align:middle; text-align:left;" | |||
!Objectives | |||
| | |||
*2.5x | |||
*10x | |||
*20x | |||
*50x | |||
| | |||
*2.5x | |||
*5x | |||
*10x | |||
*20x | |||
*50x | |||
| | |||
*5x | |||
*10x | |||
*20x | |||
*50x | |||
*100x | |||
| | |||
*2.5x | |||
*5x | |||
*10x | |||
*20x | |||
*50x | |||
| | |||
*2.5x | |||
*5x | |||
*10x | |||
*20x | |||
*50x | |||
*100x | |||
| | |||
*2.5x | |||
*5x | |||
*10x | |||
*20x | |||
*50x | |||
*100x | |||
| | |||
*2.5x | |||
*5x | |||
*10x | |||
*20x | |||
*50x | |||
*100x | |||
| | |||
*5x | |||
*10x | |||
*20x | |||
*50x | |||
*100x | |||
|Zoom 1x - 8x | |||
| | |||
*5x | |||
*10x | |||
*20x | |||
*50x | |||
| | |||
*1.25x | |||
*5xBD | |||
*10xBD | |||
*20xBD | |||
*50xBD | |||
*100xBD | |||
|- | |||
|- | |- | ||
| | |-style="background:WhiteSmoke; color:black; vertical-align:middle; text-align:left;" | ||
!Ocular | |||
|10x | |||
|10x | |10x | ||
|10x | |10x | ||
|10x | |10x | ||
|10x | |10x | ||
|10x | |10x | ||
|10x | |10x | ||
|10x | |10x | ||
| Line 91: | Line 156: | ||
|10x | |10x | ||
|- | |- | ||
| | |||
| | |- | ||
| | |-style="background:LightGrey; color:black; vertical-align:middle; text-align:left;" | ||
| | !Special<br>features | ||
| | |IR imaging | ||
| | | | ||
| | | | ||
| | | | ||
| | |||
| | |||
| | <!-- | ||
| | *Motorized stage | ||
| | *'''[[Specific_Process_Knowledge/Characterization/Optical microscope/Nikon Eclipse L200 auto scan guide|Auto scan guide]]''' | ||
| | --> | ||
| | |||
| | |||
| | |||
| | |||
|Stereoscopic | |||
| | |||
| | |||
|- | |- | ||
|- | |- | ||
| | |-style="background:WhiteSmoke; color:black; vertical-align:middle; text-align:left;" | ||
| | !Contrast<br>mechanisms | ||
| | | | ||
| | *Polarizer | ||
| | *Brightfield | ||
| | | | ||
| | *Brightfield | ||
| | *Darkfield | ||
| | | | ||
| | *Polarizer | ||
| | *Brightfield | ||
| | | | ||
*Brightfield | |||
*Darkfield | |||
| | |||
*Brightfield | |||
*Darkfield | |||
| | |||
*Polarizer | |||
*Brightfield | |||
*Darkfield | |||
| | |||
*Polarizer | |||
*Brightfield | |||
*Darkfield | |||
| | |||
*Polarizer | |||
*Brightfield | |||
*Darkfield | |||
| | |||
*Brightfield | |||
| | |||
*Brightfield | |||
*Darkfield | |||
| | |||
*Polarizer | |||
*Brightfield | |||
*Darkfield | |||
|- | |- | ||
|- | |- | ||
| | |-style="background:LightGrey; color:black; vertical-align:middle; text-align:left;" | ||
| | !Illumination<br>modes | ||
| | | | ||
| | *Episcopic | ||
| | *Diascopic | ||
| | | | ||
| | *Episcopic | ||
| | *Diascopic | ||
| | | | ||
| | *Episcopic | ||
*Diascopic | |||
| | | | ||
*Episcopic | |||
*Diascopic | |||
| | |||
*Episcopic | |||
*Diascopic | |||
| | |||
*Episcopic | |||
*Diascopic | |||
| | |||
*Episcopic | |||
*Diascopic | |||
| | |||
*Episcopic | |||
| | |||
*Episcopic | |||
| | |||
*Episcopic | |||
*Diascopic | |||
| | |||
*Episcopic | |||
*Diascopic | |||
|- | |- | ||
|- | |- | ||
| | |-style="background:WhiteSmoke; color:black; vertical-align:middle; text-align:left;" | ||
| | !Camera | ||
| | |IR camera | ||
| | |DS-Fi2 | ||
| | |None | ||
| | |DS-Fi1 | ||
| | |DS-Fi1 | ||
| | | | ||
| | *DS-Fi2 | ||
| | *C-mount,<br>0.7x relay | ||
| | | | ||
| | *DS-Fi2 | ||
*C-mount,<br>0.7x relay | |||
|DS-Fi2 | |||
|None | |||
|Infinity X | |||
| | |||
*DP23-CU | |||
*C-mount | |||
|- | |- | ||
|- | |- | ||
| | |-style="background:LightGrey; color:black; vertical-align:middle; text-align:left;" | ||
!Analysis<br>software | |||
|None | |||
| | |NIS-D | ||
| | |None | ||
| | |NIS-BR | ||
| | |NIS-D | ||
| | |NIS-D | ||
| | |NIS-D | ||
| | |NIS-D | ||
| | |None | ||
| | |DeltaPix | ||
| | |PRECiV Core | ||
| | |||
|- | |- | ||
|} | |} | ||
<br clear="all" /> | |||
There are also two optical microscopes in building 451, a stereo microscope and a transmission microscope, that were both previously located in Packlab. Please ask staff / the BioMic group for details. | |||