Jump to content

LabAdviser/314/Microscopy 314-307/Postprocessing: Difference between revisions

From LabAdviser
Jenk (talk | contribs)
Jenk (talk | contribs)
No edit summary
 
(13 intermediate revisions by 2 users not shown)
Line 1: Line 1:
<span style="background:#FF2800">THIS PAGE IS UNDER CONSTRUCTION</span>[[image:Under_construction.png|200px]]
<!-- <span style="background:#FF2800">THIS PAGE IS UNDER CONSTRUCTION</span>[[image:Under_construction.png|200px]] -->


= Available software for post-processing =
{{cc-nanolab}}
 
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/LabAdviser/314/Microscopy_314-307/Postprocessing click here]'''
 
[[Category:314]]
[[Category:314-Microscopy]]
<br>
<br>
= Access to software =
 
We have a couple of workstations available with relevant software installed. These can be accessed via [https://remote.dtu.dk remote.dtu.dk] (DTUs Citrix remote system).
 
Before being able to access, you need to write a mail to jenk@dtu.dk.
 
After you are added to the access list, follow the guide:
 
[[File:Citrix login.png|400px|thumb|left|Go to https://remote.dtu.dk and login with your DTU credentials]] <br clear="all" />
 
[[File:Citrix Apps.png|400px|thumb|left|Go to "Apps" and find the remote computers (marked with red circle in the image)]] <br clear="all" />
 
[[File:Citrix_computer-login.png|200px|thumb|left|Login with your DTU credentials]] <br clear="all" />


[[File:Citrix sign-out.png|400px|thumb|left|Remember to Sign out when done with the work. Don't save data on these PCs; all saved data during the session should be removed at the end of the session.]] <br clear="all" />


At DTU Nanolab - building 307/314 you will find a small PC lab where there is access to all the processing and productivity software available at DTU Cen. The lab is located in building 307 room 101. There are four workstations which you can access with your DTU credentials. The following software is installed on all workstations:
= Computer =
* Nlab-Ultra-data: </br>
Mainly for Spectra Ultra user.
TFS tomography software, Digital Micrograph and Velox


Microsoft Office 2016


Digital Micrograph v2 (TEM image processing and analysis)
* EDAX-OIM: </br>
EBSD/TKD user of Oxford and EDAX system. Aztec, Esprit and OIM.


TIA v4.19 (TEM/STEM image processing and analysis) (ask Cen staff for access)


JEMS v4.3905 (TEM/STEM/Diffraction analysis and simulation)
* LAB-CZC4522XC3 and LAB-CZC72977HQ: </br>
General users. Aztec, Digital micrograph, Velox


AZtec v3.3 (SEM and TEM) (EDX spectrum and map analysis)


INCA v5.0.5 (EDX analysis)
= Available software for post-processing =


Avizo v9.5 (3D rendering)


<!-- Crystalmaker v9.2.7 (Crystal structure building)
The following software is installed on the different workstations:


Crystaldiffract v6.5.5 (Diffraction analysis)


Single crystal v2.3.3 (Diffraction from single crystals) -->
Gatan GMS v3 (TEM/STEM image processing and analysis)


ThermoFisher Velox (TEM/STEM image and EDS processing and analysis)


Additionally, some of the workstations have node-locked licenses to:
ThermoFisher TIA v4.19 (TEM/STEM image processing and analysis)


PANalytical X’pert Highscore Plus (XRD data analysis): Cen-Himmelbjerg, Cen-Froebjerg, Cen-Valbybakke
Oxford AZtec v6 (EDS and EBSD analysis)


Inspect 3D (Tomography reconstruction): Cen-Himmelbjerg, Cen-Froebjerg
EDAX OIM v9 (EBSD analysis)


TrueImage v2.0.1 (TEM image reconstruction): Cen-Himmelbjerg, Cen-Froebjerg, Cen-Valbybakke, Cen-Yding
Bruker Esprit v2 (EDS and EBSD analysis)


Esprit 2.0 (EBSD, TKD and EDS, flatquad and particle analyses): Cen-Himmelbjerg, Cen-Froebjerg, Cen-Valbybakke, Cen-Yding
ThermoFisher Avizo (3D rendering)


Crystalmaker v11 (Crystal structure building)


Crystaldiffract v7 (Diffraction analysis)


Additionally, there are two workstations available in the lobby of 314. The same software is installed on these machines. One of these workstations (in front of the ATEM) is specifically made to work with large data sets created with the OneView camera of the ETEM.
Inspect 3D (Tomography reconstruction)




Please remember to log out when you have finished your work. Do not turn off the workstations.


Additionally, there is one workstation available in the lobby of 314. This has mainly Oxford Aztec available.


'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/LabAdviser/314/Postprocessing click here]'''
Please remember to log out when you have finished your work. Do not turn off the workstations.

Latest revision as of 12:33, 22 September 2026


The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.

Feedback to this page: click here

Access to software

We have a couple of workstations available with relevant software installed. These can be accessed via remote.dtu.dk (DTUs Citrix remote system).

Before being able to access, you need to write a mail to jenk@dtu.dk.

After you are added to the access list, follow the guide:

Go to https://remote.dtu.dk and login with your DTU credentials


Go to "Apps" and find the remote computers (marked with red circle in the image)


Login with your DTU credentials


Remember to Sign out when done with the work. Don't save data on these PCs; all saved data during the session should be removed at the end of the session.


Computer

  • Nlab-Ultra-data:

Mainly for Spectra Ultra user. TFS tomography software, Digital Micrograph and Velox


  • EDAX-OIM:

EBSD/TKD user of Oxford and EDAX system. Aztec, Esprit and OIM.


  • LAB-CZC4522XC3 and LAB-CZC72977HQ:

General users. Aztec, Digital micrograph, Velox


Available software for post-processing

The following software is installed on the different workstations:


Gatan GMS v3 (TEM/STEM image processing and analysis)

ThermoFisher Velox (TEM/STEM image and EDS processing and analysis)

ThermoFisher TIA v4.19 (TEM/STEM image processing and analysis)

Oxford AZtec v6 (EDS and EBSD analysis)

EDAX OIM v9 (EBSD analysis)

Bruker Esprit v2 (EDS and EBSD analysis)

ThermoFisher Avizo (3D rendering)

Crystalmaker v11 (Crystal structure building)

Crystaldiffract v7 (Diffraction analysis)

Inspect 3D (Tomography reconstruction)


Additionally, there is one workstation available in the lobby of 314. This has mainly Oxford Aztec available.

Please remember to log out when you have finished your work. Do not turn off the workstations.