Jump to content

Specific Process Knowledge/Lithography/Coaters/labspin05: Difference between revisions

From LabAdviser
Meenadh (talk | contribs)
Created page with "==Spin Coater: LabSpin 04== 400px|thumb|Spin coater: LabSpin 04 is located in PolyFabLab in building 347 Spin Coater: LabSpin 04 is a model LabSpin6 TT spin coater from SUSS. It's primary purpose is spin coating of SU-8 resist. It was installed in PolyFabLab in 2025. The user manual, user APV, and contact information can be found in [http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=547 LabManager] - '''requires login''' '''Tr..."
 
Meenadh (talk | contribs)
 
(3 intermediate revisions by the same user not shown)
Line 1: Line 1:
==Spin Coater: LabSpin 04==
==Spin Coater: LabSpin 05==
[[Image:Labspin_2.JPG|400px|thumb|Spin coater: LabSpin 04 is located in PolyFabLab in building 347]]
[[Image:Labspin_5.JPG|400px|thumb|Spin coater: LabSpin 05 is located in PolyFabLab in building 347]]


Spin Coater: LabSpin 04 is a model LabSpin6 TT spin coater from SUSS. It's primary purpose is spin coating of SU-8 resist. It was installed in PolyFabLab in 2025.
Spin Coater: LabSpin 05 is a model LabSpin6 TT spin coater from SUSS. It's primary purpose is spin coating of SU-8 resist and EBR (Edge Bead Removal) of resist on round substrates. The EBR nozzle is either fixed for 4" or 6" wafers, depending on the user's request, as it needs manual adjustment. It was installed in PolyFabLab in 2026.


The user manual, user APV, and contact information can be found in [http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=547 LabManager] - '''requires login'''
The user manual, user APV, and contact information can be found in [http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=579 LabManager] - '''requires login'''


'''Training video (same tool in Cleanroom 346): [https://www.youtube.com/watch?v=_neUkDsQhsM LabSpin02 + 03]'''
'''Training video (same tool in Cleanroom 346): [https://www.youtube.com/watch?v=_neUkDsQhsM LabSpin02 + 03]'''
Line 18: Line 18:
|style="background:LightGrey; color:black"|
|style="background:LightGrey; color:black"|
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*Spin coating of epoxy based resists
*Spin coating of epoxy-based resists
**SU-8 series
**SU-8 series
**SU-8 3000 series
**SU-8 3000 series
Line 24: Line 24:
**mr-DWL series
**mr-DWL series
*Spin coating of other resists
*Spin coating of other resists
*EBR of round substartes
|-
|-
!style="background:silver; color:black;" align="center" width="60"|Resist  
!style="background:silver; color:black;" align="center" width="60"|Resist  

Latest revision as of 12:37, 15 September 2026

Spin Coater: LabSpin 05

Spin coater: LabSpin 05 is located in PolyFabLab in building 347

Spin Coater: LabSpin 05 is a model LabSpin6 TT spin coater from SUSS. It's primary purpose is spin coating of SU-8 resist and EBR (Edge Bead Removal) of resist on round substrates. The EBR nozzle is either fixed for 4" or 6" wafers, depending on the user's request, as it needs manual adjustment. It was installed in PolyFabLab in 2026.

The user manual, user APV, and contact information can be found in LabManager - requires login

Training video (same tool in Cleanroom 346): LabSpin02 + 03

Process information

Useful information about resist dispense can be found here.

Equipment performance and process related parameters

Purpose
  • Spin coating of epoxy-based resists
    • SU-8 series
    • SU-8 3000 series
    • SU-8 XFT series
    • mr-DWL series
  • Spin coating of other resists
  • EBR of round substartes
Resist
  • manual dispense
Performance Coating thickness
  • SU-8 resists: 0.1-200 µm

Coating thickness range is dependent on specific resist formulation

Process parameters Spin speed

100 - 8000 rpm

Spin acceleration

200 - 4000 rpm/s (wrongly labelled 1/s^2 in the software)

Substrates Substrate size
  • chips, 5mm and up
  • 100 mm wafers
  • 150 mm wafers
Allowed materials

All PolyFabLab materials
See Cross Contamination Sheet in LabManager

Batch

1