Jump to content

Specific Process Knowledge/Characterization/Dektak 150: Difference between revisions

From LabAdviser
Mmat (talk | contribs)
Mmat (talk | contribs)
 
(5 intermediate revisions by the same user not shown)
Line 3: Line 3:
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/Dektak_150 click here]'''  
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Characterization/Dektak_150 click here]'''  
<br>
<br>
<br>
<br>
[[index.php?title=Category:Equipment|Characterization Profiler]]
[[Category:Equipment|Characterization Profiler]]
[[index.php?title=Category:Characterization|Profiler]]
[[Category:Characterization|Profiler]]


= Stylus Profiler: Dektak150 =
= Dektak150 (Stylus Profiler) =
[[image:Dektak150.JPG|300x300px|right|thumb|Stylus profiler:Dektak150, currently located in building 451, room 913 (as of 2023).]]
[[image:Dektak150.JPG|300x300px|right|thumb|Stylus profiler:Dektak150, currently located in building 451, room 913 (as of 2023).]]


Line 14: Line 13:




'''The user manual, technical information and contact information can be found in LabManager:'''
The user manual, technical information and contact information can be found in [http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=457 LabManager].
 
[http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=457 Stylus profiler:Dektak150 in LabManager]


The computer is not connected to the network but data can be saved on a dedicated USB and transfered to a computer on the network.
The computer is not connected to the network but data can be saved on a dedicated USB and transfered to a computer on the network.


Info about measurement accuracy can be found [[/Stylus profiler measurement uncertainty|here]].
We have currently no verified information about the measurement accuracy/uncertainity for this profilometer, but only for the [https://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Characterization/Stylus_Profiler_Measurement_Uncertainty Dektak XTA].
 
<br>
===Equipment performance and process related parameters===
<br>
===Performance and Process Parameters===


{| border="2" cellspacing="0" cellpadding="10"  
{| border="2" cellspacing="0" cellpadding="10"  

Latest revision as of 15:26, 6 August 2026

The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.

Feedback to this page: click here

Dektak150 (Stylus Profiler)

Stylus profiler:Dektak150, currently located in building 451, room 913 (as of 2023).

The stylus profiler Dektak150 is intended for profile measurements on samples outside the cleanroom. The Dektak150 is especially well suited for measuring soft samples as it can be adjusted to apply lower force than the other stylus profilers at Nanolab.


The user manual, technical information and contact information can be found in LabManager.

The computer is not connected to the network but data can be saved on a dedicated USB and transfered to a computer on the network.

We have currently no verified information about the measurement accuracy/uncertainity for this profilometer, but only for the Dektak XTA.

Performance and Process Parameters

Purpose Profiler for measuring micro structures|
  • Single line profiles
  • Surface roughness on a line scan
Location Building 347, room 080
  • North-East corner of the building, in the basement
  • When you enter the building from the East, you enter directly into the basement.
Performance Scan range x y

Line scan x: 50 µm to 55 mm in a single scan

Scan range z

50 Å to 1 mm

Resolution x y

Theoretically down to 0.003 µm (in practice the resolution is limited by the tip size)

Resolution z

1Å (@65kÅ), 10Å (@655 kÅ), 80 Å (@5240 kÅ), 160 Å (@1mm)

Maximum sample thickness

100 mm

Hardware settings Tip radius
  • 5 µm 45o cone
  • 0.2 µm 45o cone on request
Substrates Substrate size
  • Up to 6"
Substrate materials allowed
  • In principle all materials