Specific Process Knowledge/Lithography/UVExposure/aligner MA6-1: Difference between revisions
No edit summary |
|||
| (One intermediate revision by the same user not shown) | |||
| Line 13: | Line 13: | ||
|- | |- | ||
! style="text-align:left" | Location: | ! style="text-align:left" | Location: | ||
| style="padding-left: 10px" | | | style="padding-left: 10px" | PolyFabLab | ||
|} | |} | ||
| Line 83: | Line 83: | ||
==Alignment mark design and locations== | ==Alignment mark design and locations== | ||
[[Specific_Process_Knowledge/Pattern_Design#Alignment_marks|Alignment mark design and locations]]. | [[Specific_Process_Knowledge/Pattern_Design#Alignment_marks|Alignment mark design and locations]]. | ||
Latest revision as of 12:46, 26 June 2026
Aligner: MA6-1

Tool description
The Aligner: MA6-1 is a manual UV exposure system, which can be used for mask alignment and exposure of UV resists on 100 mm substrates. It is also capable of flood exposing chips, 50 mm and 150 mm substrates.
| Product: | Süss mask aligner MA6 |
|---|---|
| Year of purchase: | 1999 |
| Location: | PolyFabLab |
User manual
The user manual and contact information can be found in LabManager - requires login
Tool training
Training on the tool requires users to complete the lithography TPT followed by reading the manual and watching the training videos. The tool authorization can be obtained after a successful hands-on authorization training session.
The training videos were made for MA6-2, but operation of MA6-1 is very similar as they are exactly the same model. Due to a different power supply, however, procedures for ignition and intensity control of the lamp is different for MA6-1. Please refer to the manual for the correct procedures.
| Purpose | Mask alignment and UV exposure |
|---|---|
| Exposure modes |
|
| Exposure light/filters |
|
| Minimum resolution | ~1.25 µm |
| Mask size | 5x5 inches |
| Alignment modes |
|
| Substrate size |
|
| Allowed materials | All PolyFabLab allowed materials |
| Substrate batch | 1 |
Process information
The Aligner: MA6-1 has an i-line notch filter installed. This results in an exposure light peak around 365nm with a FWHM of 7nm.
Exposure dose
Information on UV exposure dose