Jump to content

LabAdviser/Courses: Difference between revisions

From LabAdviser
Mmat (talk | contribs)
Reet (talk | contribs)
 
(27 intermediate revisions by 3 users not shown)
Line 6: Line 6:


= Tool Package Training (TPT) =
= Tool Package Training (TPT) =
For selected equipment groups, we create online introductory courses called Tool Package Training (TPT) that provide a comprehensive overview of both the theoretical principles behind the processes and the equipment used. These courses also include video demonstrations showcasing the operation of the equipment available in our cleanroom facilities. The completion of the respective TPTs are mandatory for all academic users before hands-on training on specific equipment can be requested. While we strongly recommend commercial users to take the online courses as well, only the video demonstrations showcasing the operation of the equipment are mandatory.
For selected equipment groups, we have created online introductory courses called Tool Package Training (TPT) that provide a comprehensive overview of both the theoretical principles behind the processes and the equipment used. These courses also include video demonstrations showcasing the operation of the equipment available in our cleanroom facilities. The completion of the respective TPTs are mandatory for all academic users before hands-on training on specific equipment can be requested. While we strongly recommend commercial users to take the online courses as well, only the video demonstrations showcasing the operation of the equipment are mandatory.


{| border="1" cellspacing="1" cellpadding="3" style="text-align:left;"  
{| border="1" cellspacing="1" cellpadding="3" style="text-align:left;"  
Line 31: Line 31:
!SEM TPT
!SEM TPT
|for getting access to SEMs in [https://labadviser.nanolab.dtu.dk//index.php?title=Specific_Process_Knowledge/Characterization/SEM:_Scanning_Electron_Microscopy 346] and [https://labadviser.nanolab.dtu.dk/index.php?title=LabAdviser/314/Microscopy_314-307 314/307]
|for getting access to SEMs in [https://labadviser.nanolab.dtu.dk//index.php?title=Specific_Process_Knowledge/Characterization/SEM:_Scanning_Electron_Microscopy 346] and [https://labadviser.nanolab.dtu.dk/index.php?title=LabAdviser/314/Microscopy_314-307 314/307]
|This online course presents the theory about scanning electron microscopy, as well as training in equipment operation. The course is a prerequisite for hands-on training on any of the SEMs in building 314/307, and 346 at DTU Nanolab. Find more information on the [https://labadviser.nanolab.dtu.dk/index.php?title=LabAdviser/Courses/TPT_SEM SEM TPT] and sign up [https://www.nanolab.dtu.dk/access/cleanroom-access/equipment-training/scanning-electron-microscopy-sem here].  
|This online course presents the theory about scanning electron microscopy, as well as training in equipment operation. The course is a prerequisite for hands-on training on any of the SEMs in building 314/307, and 346/347 at DTU Nanolab. Find more information on the [https://labadviser.nanolab.dtu.dk/index.php?title=LabAdviser/Courses/TPT_SEM SEM TPT] and sign up [https://www.nanolab.dtu.dk/access/cleanroom-access/equipment-training/scanning-electron-microscopy-sem here].  
|-
|-
|}
|}
Line 46: Line 46:
|-
|-
|- style="background:LightGrey; color:black" valign="center"
|- style="background:LightGrey; color:black" valign="center"
!E-beam Lithography Tutorial
! E-beam Evaporators
| for getting access to the E-beam Evaporator [[Specific Process Knowledge/Thin film deposition/Temescal | Temescal]] or [[Specific Process Knowledge/Thin film deposition/10-pocket e-beam evaporator | 10-pocket E-beam Evaporator]]
|This online course consists of four short training videos regarding equipment operation for both tools. 
* [https://learn.inside.dtu.dk/d2l/le/lessons/312055/lessons/1163908 E-beam Evaporator Training videos in DTU Learn]
* [https://www.youtube.com/playlist?list=PLjWVU97LayHCQWuQyHwddJnpsEYfQp0wf same videos on Youtube]
|-
|- style="background:WhiteSmoke; color:black" valign="center"
!E-beam Lithography
|for getting access to [[Specific Process Knowledge/Lithography/EBeamLithography | E-beam Lithography Tools]]
|for getting access to [[Specific Process Knowledge/Lithography/EBeamLithography | E-beam Lithography Tools]]
|This online tutorial will be part of the E-beam TPT and is currently under prepration. <!-- ADDED WHEN TPT IS READY: It will include theory on electron beam lithography and equipment, as well as training in preparation of  exposure files and equipment operation.!--> The course is a prerequisite for hands-on training on the electron beam tool. Find more information on the [[LabAdviser/Courses/TPT Ebeam|E-beam Tutorial]] and request training via [mailto:training@nanolab.dtu.dk training@nanolab.dtu.dk].
|This online tutorial will be part of the E-beam TPT and is currently under prepration. <!-- ADDED WHEN TPT IS READY: It will include theory on electron beam lithography and equipment, as well as training in preparation of  exposure files and equipment operation.!--> The course is a prerequisite for hands-on training on the electron beam tool. Find more information about the training in the [[LabAdviser/Courses/TPT Ebeam|TPT E-beam]].  
|-
|-
|- style="background:WhiteSmoke; color:black" valign="center"
|- style="background:LightGrey; color:black" valign="center"
!Ellipsometer Tutorial
!Ellipsometer VASE
|for getting access to the [[Specific Process Knowledge/Characterization/Optical characterization#Ellipsometer VASE and Ellipsometer M-2000V|Ellipsometers]]
|for getting access to the [[Specific Process Knowledge/Characterization/Optical characterization#Ellipsometer VASE and Ellipsometer M-2000V|Ellipsometers]]
|This online course consists of two short online tutorials  
|This online course consists of two short online tutorials  
* [https://www.jawoollam.com/resources/ellipsometry-tutorial/what-is-ellipsometry  Tutorial by ''Woollam'']
* [https://www.jawoollam.com/resources/ellipsometry-tutorial/what-is-ellipsometry  Tutorial ''by Woollam'']
* [https://www.youtube.com/watch?v=EC-oyRhKr0A|Ellipsometer Equipment operation by ''DTU Nanolab'']
* [https://www.youtube.com/watch?v=EC-oyRhKr0A|Ellipsometer Ellipsometer operation ''by DTU Nanolab'']
|-
|- style="background:WhiteSmoke; color:black" valign="center"
! Atomic Force Microscopy
| for getting access to the [[Specific Process Knowledge/Characterization/AFM:_Atomic_Force_Microscopy | AFM equipment]]
|This online course consists of three short training videos regarding equipment operation. 
* [https://www.youtube.com/watch?v=i6JXopjBiy4&list=PLjWVU97LayHC9xeoG2uv8IaHuY7t-q0Tj AFM Icon-PT Operation]
|-
|-
|- style="background:LightGrey; color:black" valign="center"
|- style="background:LightGrey; color:black" valign="center"
! AFM Tutorial
! Lesker Dual Chamber Sputter System
| for getting access to the [[Specific Process Knowledge/Characterization/AFM:_Atomic_Force_Microscopy]]
| for getting access to the [[Specific Process Knowledge/Thin film deposition/Cluster-based multi-chamber high vacuum sputtering deposition system | Sputter-System Metal-Oxide(PC1) Metal-Nitride (PC3)]]
|This online course consists of 3 short training videos regarding equipment operation. The course is a prerequisite for hands-on training on AFM equipment in building 346.  
|This online course consists of three short training videos regarding equipment operation for PC1 (Oxide) and PC3 (Nitride)).
[https://www.youtube.com/watch?v=i6JXopjBiy4&list=PLjWVU97LayHC9xeoG2uv8IaHuY7t-q0Tj AFM Icon-PT training videos by ''DTU Nanolab'']
* [https://www.youtube.com/watch?v=1WHv36coRUc PC1 (Oxide) and PC3 (Nitride) Operation]
|-
|-
|- style="background:WhiteSmoke; color:black" valign="center"
! XPS
| for getting access to the [[Specific Process Knowledge/Characterization/XPS | XPS]]
|If you already a user at DTU Nanolab and have access to LabManager, please fill the access request form following the link below:
*[http://labmanager.dtu.dk/function.php?module=Request&view=edit&rt=2 Access request form for XPS training]
Else, please contact the Fabrication Support group.
 
This online course presents the theory behind XPS analysis, as well as training in equipment operation in the cleanroom.
* "Theory behind XPS" by ''Technical University of Munich'' (pages 1-16): [[File:Electron Spectroscopy of surfaces.pdf]]
* Youtube video by ''Kent L. Rhodes (McCrone Group)'' hosted by ''Hooke College of Applied Sciences'': [https://www.youtube.com/watch?v=nGQxmOcs2rg "Using XPS for Industrial Problem Solving"]
* Equipment operation by DTU Nanolab:
: [https://www.youtube.com/playlist?list=PLjWVU97LayHBtOkPCSv8QA-sD4Dbz1jrb XPS Operation]
|-
|-
|}
|}
Line 72: Line 99:
<br>
<br>
<br clear="all">
<br clear="all">
=Links to Training Videos=
DTU Nanolab has a YouTube channel where we have gathered all our training videos: [https://www.youtube.com/channel/UCJhdUTUJRDNODNiC3V95RQQ]
We have a number of playlists and some single videos for equipment. You can get an overview here with links to the playlists/videos on You Tube
==Safety and Behavior==
*Nanolab introduction course: Safety in the Cleanroom [https://www.youtube.com/watch?v=Dfu66Ewu4as&t=606s]
*Cleanroom safety at DTU Nanolab [https://www.youtube.com/watch?v=3MoKP1E1LGs&t=5s]
*Working with chemicals in the cleanroom at DTU Nanolab [https://www.youtube.com/watch?v=txmgMZReY80]
*Behaviour in the cleanroom at DTU Nanolab [https://www.youtube.com/watch?v=ROWObpRQFZ8]
*Playlist: Craftsmen in the cleanroom/håndværkere i renrummet. [https://www.youtube.com/watch?v=D-0T9X9FFBQ&list=PLjWVU97LayHDKnUd0GrKXdqDhRZuI3iwW]
==Labmanager and Labadviser==
*Playlist: DTU Nanolab systems (Labmanager and Labadviser)[https://www.youtube.com/watch?v=jC5soGfyrZc&list=PLjWVU97LayHA_ZKxvmNfTg1Bp53GX07ER]
==Wet Chemistry==
*Training in fume hoods part 1 - Intro and Getting Started [https://www.youtube.com/watch?v=DRPHtBAqpU0]
*Training in fume hoods part 2 - Working With Acids, Bases and Solvents [https://www.youtube.com/watch?v=sqqktgLklSs]
*Training in fume hoods part 3 – Wet benches and errors [https://www.youtube.com/watch?v=bvK1ONO1lwM]
*Using Quick Dump Rinse Baths [https://www.youtube.com/watch?v=edMt18Uwq9o&list=PLjWVU97LayHCS7pcUsx1qt7vroSdHciXV]
*Native Silicon Dioxide Removal [https://www.youtube.com/watch?v=4JD-fSWlZac]
==Lithography==
* Playlist: Lithography TPT - lecture videos [https://www.youtube.com/playlist?list=PLjWVU97LayHCp7x9OujmVlZWLAnK4CDFR]
* Playlist: Lithography TPT - tool training (Spin Coater, Mask Aligner MA6-2, Automatic Puddle Developer) [https://www.youtube.com/watch?v=3JhM3rmLVpA&list=PLjWVU97LayHCX4sz2AH_YiPbNRmkrBYe5]
* Playlist: Lithography TPT - tool training (Maskless Aligner) [https://www.youtube.com/watch?v=GyTQNmbev2c&list=PLjWVU97LayHAiCabstMfAUeeWyQoQI_cV]
* E-beam lithography at DTU Nanolab [https://www.youtube.com/watch?v=2bFUO201DS4]
* JEOL 9500 EBL [https://youtu.be/-wZpUNAq8dA?si=UCWm9rL5SoJE9t1I]
* Manual Spin Coater: Labspin [https://www.youtube.com/watch?v=_neUkDsQhsM]
* Manual Puddle Developer [https://www.youtube.com/watch?v=btinNzYnLnY&t=2s]
==Thin Film Deposition and Oxidation==
*Playlist: E-beam evaporator (Temescal) [https://www.youtube.com/watch?v=XNvnv4R8a5o&list=PLjWVU97LayHCQWuQyHwddJnpsEYfQp0wf]
*Lesker dual chamber sputter system at DTU Nanolab [https://www.youtube.com/watch?v=1WHv36coRUc]
*Antistiction treatment [https://www.youtube.com/watch?v=5NrPWXVybXg]
* Furnace training: Oxidation furnace [https://www.youtube.com/watch?v=Hi-1zN1RVqc]
==Dry Etch==
*Playlist: Dry Etch TPT - Lecture videos [https://www.youtube.com/watch?v=6k6QUyDKQQc&list=PLjWVU97LayHBu0XwMGHss5CdEhka6B72U]
*Playlist: Dry Etch TPT - hands-on videos [https://www.youtube.com/watch?v=ovNM4A4E8Q0&list=PLjWVU97LayHC9cl0cuB65m-FlIScBd5t9]
==Characterization==
*Playlist: SEM Training videos for Zeiss Supra SEMs in building 346 [https://www.youtube.com/watch?v=JuFZUsbSHvQ&list=PLjWVU97LayHAIltgr7pUoeIkwiPuP4Qsj]
*Playlist: AFM Icon Nanoscope software training part I/II/III [https://www.youtube.com/watch?v=i6JXopjBiy4&list=PLjWVU97LayHC9xeoG2uv8IaHuY7t-q0Tj]
*Ellipsometer training [https://www.youtube.com/watch?v=EC-oyRhKr0A]
*Playlist: XPS [https://www.youtube.com/playlist?list=PLjWVU97LayHBtOkPCSv8QA-sD4Dbz1jrb]
==Backend Tools==
* Disco Dicing saw - blade exchange [https://www.youtube.com/watch?v=0pMraXlfqh8]

Latest revision as of 11:44, 23 April 2026

The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.

Feedback to this page: click here


Tool Package Training (TPT)

For selected equipment groups, we have created online introductory courses called Tool Package Training (TPT) that provide a comprehensive overview of both the theoretical principles behind the processes and the equipment used. These courses also include video demonstrations showcasing the operation of the equipment available in our cleanroom facilities. The completion of the respective TPTs are mandatory for all academic users before hands-on training on specific equipment can be requested. While we strongly recommend commercial users to take the online courses as well, only the video demonstrations showcasing the operation of the equipment are mandatory.

Course Requirement Description
Lithography TPT for working with Lithography Equipment This online course presents the theory on lithographic processes and equipment, as well as training in equipment operation in the cleanroom. The course is a prerequisite for hands-on training on all lithography equipment. Find more information on the Lithography TPT and sign up here.
Thin Film TPT for getting access to Thin Film Deposition & Thermal Growth Equipment This online course introduces the theory for thin film growth and deposition techniques available at DTU Nanolab. The course is a prerequisite for hands-on training on most of the thin film equipment in the cleanroom. Find more information on the Thin Film TPT and sign up here.
Dry Etch TPT for getting access to Dry Etch Equipment This online course presents the theory on dry etching and equipment, as well as training in equipment operation. The course is a prerequisite for hands-on training on any of the dry etching equipment in the cleanroom. Find more information on the Dry Etch TPT and sign up here
SEM TPT for getting access to SEMs in 346 and 314/307 This online course presents the theory about scanning electron microscopy, as well as training in equipment operation. The course is a prerequisite for hands-on training on any of the SEMs in building 314/307, and 346/347 at DTU Nanolab. Find more information on the SEM TPT and sign up here.



Equipment Tutorials

For selected equipment, we have created online courses called exxplaining the operation (hardware and software) of our equipment. These tutorials are mandatory for all users before hands-on training on specific equipment can be requested via training@nanolab.dtu.dk.

Course Requirement Description
E-beam Evaporators for getting access to the E-beam Evaporator Temescal or 10-pocket E-beam Evaporator This online course consists of four short training videos regarding equipment operation for both tools.
E-beam Lithography for getting access to E-beam Lithography Tools This online tutorial will be part of the E-beam TPT and is currently under prepration. The course is a prerequisite for hands-on training on the electron beam tool. Find more information about the training in the TPT E-beam.
Ellipsometer VASE for getting access to the Ellipsometers This online course consists of two short online tutorials
Atomic Force Microscopy for getting access to the AFM equipment This online course consists of three short training videos regarding equipment operation.
Lesker Dual Chamber Sputter System for getting access to the Sputter-System Metal-Oxide(PC1) Metal-Nitride (PC3) This online course consists of three short training videos regarding equipment operation for PC1 (Oxide) and PC3 (Nitride)).
XPS for getting access to the XPS If you already a user at DTU Nanolab and have access to LabManager, please fill the access request form following the link below:

Else, please contact the Fabrication Support group.

This online course presents the theory behind XPS analysis, as well as training in equipment operation in the cleanroom.

XPS Operation