Jump to content

Specific Process Knowledge/Thermal Process/C3 Anneal-bond furnace: Difference between revisions

Paphol (talk | contribs)
No edit summary
Pevo (talk | contribs)
 
(3 intermediate revisions by 2 users not shown)
Line 1: Line 1:
{{cc-nanolab}}
'''Feedback to this page''': '''[mailto:thinfilm@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thermal_Process/C3_Anneal-bond_furnace click here]'''
'''Feedback to this page''': '''[mailto:thinfilm@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thermal_Process/C3_Anneal-bond_furnace click here]'''


''This page is written by DTU Nanolab  internal''
 
[[Category: Equipment |Thermal C3]]
[[index.php?title=Category:Equipment|Thermal C3]]
[[Category: Thermal process|C3]]
[[index.php?title=Category:Thermal process|C3]]
[[Category: Furnaces|C3]]
[[index.php?title=Category:Furnaces|C3]]


==Anneal-bond furnace (C3)==
==Anneal-bond furnace (C3)==
Line 42: Line 44:
|-
|-
!style="background:silver; color:black" align="center"|Performance
!style="background:silver; color:black" align="center"|Performance
|style="background:LightGrey; color:black"|Film thickness
|style="background:LightGrey; color:black"|Film thickness and quality
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*Dry oxide:~ 0 nm  to 300 nm (it takes too long to grow thicker dry oxide layers)
*Dry oxide:~ 0 nm  to 300 nm (it takes too long to grow thicker dry oxide layers)
*Wet oxide: ~ 0 nm to 3 µm (23 hours wet oxidation at 1100 <sup>o</sup>C)
*Wet oxide: ~ 0 nm to 3 µm (23 hours wet oxidation at 1100 <sup>o</sup>C)
* [[Specific Process Knowledge/Thermal Process/Oxidation/Breakdown voltage measurements/C3 furnace break-down voltage measurement results|Break-down voltage measurement results]]
|-
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="3"|Process parameter range
!style="background:silver; color:black" align="center" valign="center" rowspan="3"|Process parameter range
Line 70: Line 73:
*Silicon wafers  
*Silicon wafers  
*Silicon wafers with layers of silicon oxide or silicon nitride  
*Silicon wafers with layers of silicon oxide or silicon nitride  
*Wafers from the LPCVD furnaces
*Wafers from the A1, A3, B-stack, C1 and E1 stack furnaces
*Wafers from PECVD4
*Wafers and samples from PECVD4
*Wafers from PECVD3 (without any metal)
*Wafers and samples from PECVD3 (without any metals)
*Wafers from Wafer Bonder 02 (assuming they were clean and not have been exposed to any metal when entering the Wafer Bonder 02)
*Wafers from Wafer Bonder 02
*Wafers from Wafer Bonder 03 (without any metals). Use new or dedicated/clean teflon sheets in the wafer bonder
|-  
|-  
|}
|}