!style="background:silver; color:black;" align="left"|Purpose  
!style="background:silver; color:black;" align="left"|Purpose  
|style="background:LightGrey; color:black"|Deposition of various materials ||style="background:WhiteSmoke; color:black"|
|style="background:LightGrey; color:black"|Deposition of various materials ||style="background:WhiteSmoke; color:black"|
*Sputtering of metals including alloys and magnetic metals, semiconductors including silicon, and some dielectrica. See tables above and ask staff if there is a material you would like to deposit which you do not see listed.
* Metals including alloys and magnetic materials
* Dielectrica including silica and alumina.  
* Semiconductors including silicon
* See tables above and ask staff if there is a material you would like to deposit which you do not see listed.
|-
|-
!style="background:silver; color:black" align="left" valign="top" rowspan="2"|Performance
!style="background:silver; color:black" align="left" valign="top" rowspan="2"|Performance
Line 345: Line 348:
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*Ar
*Ar
*N<math>_2</math>
*N<sub>2</sub>
*O<math>_2</math>
*O<sub>2</sub>
*2%O<math>_2</math> in Ar
*2 % O<sub>2</sub> in Ar
* mixtures of the above
* mixtures of the above
|-
|-
Line 360: Line 363:
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*Silicon wafers
*Silicon wafers
*and almost any other
*and almost any other as long as it does not degas.
*See cross-contamination sheet [https://labmanager.dtu.dk/function.php?module=XcMachineaction&view=edit&MachID=244]
|-  
|-  
| style="background:LightGrey; color:black"|Material allowed on the substrate
| style="background:LightGrey; color:black"|Material allowed on the substrate
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*almost any  
*almost any as long as it does not degas.
|-  
|-  
|}
|}
==Maximum Power Calculation==
* <math>PD</math> - Power density (fundamental constant given by a supplier)
* <math>P(W)</math> - Power (W) from power supply
* <math>A(inch^2)</math> - Area of the target
------------------------------------------------------------------------------------------------------------
<math> PD=\frac{P(W)}{A(inch^2)}</math>  &#8658;    <math>P(W)=PD\cdot A(inch^2)=PD\cdot\frac{\pi d^2}{4}</math>
<ul>
<li><p> <b><span style="color: green">d=2" (2-inch target)</span></b> <math>P(W)=3.14\cdot PD</math>  </p></li>
<li><p> <b><span style="color: green">d=3" (3-inch target)</span></b> <math>P(W)=7.065\cdot PD</math>  </p></li>
<li><p> <b><span style="color: green">d=4" (4-inch target)</span></b> <math>P(W)=12.56\cdot PD</math>  </p></li>
<li><p> <b><span style="color: green">d=6" (6-inch target)</span></b> <math>P(W)=28.26\cdot PD</math>  </p></li>
</ul>
--------------------------------------------------
Value of the <math>PD</math> is material dependent and can be found on KJLC homepage