== Studies of Cr deposition processes ==
== Studies of Cr deposition processes ==


[[/Deposition of Chromium|Uniformity of Cr layers]] - ''Uniformity of Cr layers deposited with different methods and settings''
[[/Roughness of Chromium|Roughness of Chromium]] - ''Roughness and Uniformity of Cr layers deposited with different methods and settings''
 
[[/Sputtering of Cr in Wordentec|Sputtering of Cr in Wordentec]] - ''Settings and deposition rates''


[[/Sputtering of Cr in Sputter System (Lesker)|Sputtering of Cr in Sputter system (Lesker)]] - ''Settings and deposition rates''
[[/Sputtering of Cr in Sputter System (Lesker)|Sputtering of Cr in Sputter system (Lesker)]] - ''Settings and deposition rates''
Line 18: Line 16:


[[Specific_Process_Knowledge/Thin_film_deposition/Lesker/Stress_dependence_on_sputter_parameters_in_the_Lesker_sputter_system#Cr:_High_tensile_stress|Stress in sputtered Cr films]] - ''Extremely high tensile stress in Cr films deposited at high temperature''
[[Specific_Process_Knowledge/Thin_film_deposition/Lesker/Stress_dependence_on_sputter_parameters_in_the_Lesker_sputter_system#Cr:_High_tensile_stress|Stress in sputtered Cr films]] - ''Extremely high tensile stress in Cr films deposited at high temperature''


== Chromium deposition ==
== Chromium deposition ==
Line 69: Line 66:


|
|
Up to *3x 4" wafers or
*Up to *3x 4" wafers or
*1x6" or 1x 8" wafer
*1x6" or 1x 8" wafer
*Many smaller samples
*Many smaller samples
Line 107: Line 104:


|}  
|}  
'''*''' ''For thicknesses above 300 nm, please request permission from metal@nanolab.dtu.dk to ensure there is enough material.''
'''*''' ''For thicknesses above 300 nm, please request permission from metal@nanolab.dtu.dk to ensure there is enough material and to prioritize chamber cleaning as Cr tends to be a high-stress layer and thus causes flaking,''