Jump to content

Specific Process Knowledge/Thermal Process: Difference between revisions

From LabAdviser
Pevo (talk | contribs)
Pevo (talk | contribs)
 
(6 intermediate revisions by 2 users not shown)
Line 1: Line 1:
{{cc-nanolab}}
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thermal_Process click here]'''  
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thermal_Process click here]'''  
''This page is written by DTU Nanolab  internal''




Line 16: Line 16:
'''A stack furnaces:'''
'''A stack furnaces:'''
*[[/A1 Bor Drive-in furnace|Boron Drive-in + Predep furnace (A1)]] - ''For oxidation and annealing of Si wafers, and for boron pre-deposition (doping) and for drive-in afterwards''
*[[/A1 Bor Drive-in furnace|Boron Drive-in + Predep furnace (A1)]] - ''For oxidation and annealing of Si wafers, and for boron pre-deposition (doping) and for drive-in afterwards''
*[[/A2 Gate Oxide furnace|Gate Oxide furnace (A2)]] - Not in use
*[[/A2 Gate Oxide furnace|Gate Oxide furnace (A2)]] - ''For dry oxidation of Si wafers''
*[[/A3 Phosphor Drive-in furnace|Phosphorus Drive-in furnace (A3)]] - ''For oxidation and annealing of Si wafers and for drive-in after phosphorus pre-dep''
*[[/A3 Phosphor Drive-in furnace|Phosphorus Drive-in furnace (A3)]] - ''For oxidation and annealing of Si wafers and for drive-in after phosphorus pre-dep''
*[[/A4 Phosphor Pre-dep furnace|Phosphorus Predep furnace (A4)]] - ''For pre-deposition (doping) of phosphorus on Si wafers''  
*[[/A4 Phosphor Pre-dep furnace|Phosphorus Predep furnace (A4)]] - ''For pre-deposition (doping) of phosphorus on Si wafers''  
Line 22: Line 22:
'''C stack furnaces:'''
'''C stack furnaces:'''
*[[/C1 Furnace Anneal-oxide|Anneal-oxide furnace (C1)]] - ''For oxidation and annealing of 100 mm and 150 mm wafers''
*[[/C1 Furnace Anneal-oxide|Anneal-oxide furnace (C1)]] - ''For oxidation and annealing of 100 mm and 150 mm wafers''
*[[/C2 Furnace III-V oxidation |III-V oxidation furnace (C2)]] - ''For oxidation of Al<sub>x</sub>GaAs layers.''
*[[/C2 Furnace General Purpose Annealing|General Purpose Annealing furnace (C2)]] - ''For annealing of different samples and materials.''
*[[/C3 Anneal-bond furnace|Anneal-bond furnace (C3)]] - ''For oxidation and annealing of bonded wafers''
*[[/C3 Anneal-bond furnace|Anneal-bond furnace (C3)]] - ''For oxidation and annealing of bonded wafers''
*[[/C4 Aluminium Anneal furnace|Aluminium Anneal furnace (C4)]] - ''For annealing and oxidation of wafers containing e.g. aluminium, Al<sub>2</sub>O<sub>3</sub> and TiO<sub>2</sub> ''
*[[/C4 Aluminium Anneal furnace|Aluminium Anneal furnace (C4)]] - ''For annealing and oxidation of wafers containing e.g. aluminium, Al<sub>2</sub>O<sub>3</sub> and TiO<sub>2</sub> ''

Latest revision as of 14:01, 27 May 2025

The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.

Feedback to this page: click here


Choose a process type

Choose an equipment to use

A stack furnaces:

C stack furnaces:

E stack furnaces:

Other furnaces:

Rules for storage and RCA cleaning of wafers to the A and C stack furnaces


Manual for the furnace computer to the A, B, C and E stack furnaces

The A, B, C and E stack furnaces can be controlled either from a touch screen by each furnace or from a furnace computer. The user manual for the furnace computer can be found here in LabManager (login required):

Decommissioned equipment