'''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.''' | |||
'''All links to Kemibrug (SDS) and Labmanager Including APV and QC requires login.''' | |||
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Etching_of_Platin click here]''' | |||
[[Category: Equipment|Etch Wet Platinum]] | |||
[[Category: Etch (Wet) bath|Platinum]] | |||
==Etching of Platinum== | |||
Etching of Platinum can be done either by wet etch or by sputtering with ions. | |||
*[[Specific Process Knowledge/Etch/Wet Platinum Etch|Etching of Platinum by wet etch]] | |||
*[[Specific_Process_Knowledge/Etch/IBE⁄IBSD Ionfab 300|Sputtering of Pt]] | |||
Etching of | |||
*[[Specific Process Knowledge/Etch/Wet | |||
*[[Specific_Process_Knowledge/Etch/IBE⁄IBSD Ionfab 300 | |||
<br clear="all" /> | <br clear="all" /> | ||
==Comparison of | ==Comparison of Platinum Etch Methods== | ||
{|border="1" cellspacing="1" cellpadding="3" style="text-align:left;" | {|border="1" cellspacing="1" cellpadding="3" style="text-align:left;" | ||
| Line 22: | Line 23: | ||
|-style="background:silver; color:black" | |-style="background:silver; color:black" | ||
! | ! | ||
![[Specific Process Knowledge/Etch/Wet | ![[Specific Process Knowledge/Etch/Wet Platinum Etch|Pt wet etch]] | ||
![[Specific_Process_Knowledge/Etch/IBE⁄IBSD Ionfab 300|IBE (Ionfab300+)]] | ![[Specific_Process_Knowledge/Etch/IBE⁄IBSD Ionfab 300|IBE (Ionfab300+)]] | ||
|- | |- | ||
| Line 30: | Line 30: | ||
|-style="background:WhiteSmoke; color:black" | |-style="background:WhiteSmoke; color:black" | ||
!Generel description | !Generel description | ||
|Wet etch of | |Wet etch of Pt | ||
|Sputtering of Pt | |||
|Sputtering of | |||
|- | |- | ||
| Line 39: | Line 38: | ||
!Etch rate range | !Etch rate range | ||
| | | | ||
*~ | *~ 1 - 10 nm/min (not tested yet) | ||
| | | | ||
*~ | *~30nm/min (not tested yet) | ||
|- | |- | ||
| Line 49: | Line 46: | ||
|-style="background:WhiteSmoke; color:black" | |-style="background:WhiteSmoke; color:black" | ||
!Etch profile | !Etch profile | ||
| | | | ||
*Isotropic | *Isotropic | ||
| Line 60: | Line 55: | ||
!Masking material | !Masking material | ||
| | | | ||
*None (only used for stripping Pt) | |||
*None (only used for | |||
| | | | ||
*Any material that is allowed in the chamber, photoresists included | *Any material that is allowed in the chamber, photoresists included | ||
| Line 72: | Line 65: | ||
!Substrate size | !Substrate size | ||
| | | | ||
*Any size and number that can go inside the beaker in use | *Any size and number that can go inside the beaker in use | ||
| | | | ||
Smaller pieces glued to carrier wafer | Smaller pieces glued to carrier wafer | ||
| Line 88: | Line 78: | ||
!'''Allowed materials''' | !'''Allowed materials''' | ||
| | | | ||
No restrictions cross contamination wise as long as you use the right beaker and make sure that they are safe to enter in the chemicals | No restrictions cross contamination wise as long as you use the right beaker and make sure that they are safe to enter in the chemicals | ||
| | | | ||
*Silicon | *Silicon | ||