Jump to content

Specific Process Knowledge/Back-end processing/Micro transfer printer: Difference between revisions

From LabAdviser
Jehem (talk | contribs)
No edit summary
Meenadh (talk | contribs)
 
(20 intermediate revisions by 2 users not shown)
Line 4: Line 4:


[[Category: Equipment|Backend]]
[[Category: Equipment|Backend]]
[[Category: Bckend]]
[[Category: Backend]]


__TOC__
=Micro Transfer Printer=


Micro transfer printing is an emerging technique to transfer diverse and non-native components from source substrate to target substrate. Micro transfer printing is best for achieving heterogeneous integration,
where micro-components from different sources are picked up by polymer stamp and precisely assembled onto different target substrate such as glass, plastic, ceramic and silicon. This method is known for
increasing functionality and improving efficiency.


__TOC__
Micro transfer printer 1003 from Xdisplay was installed in year 2022 and placed in cleanroom F-4.
 
Equipment info in [http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=503 Lab Manager] - '''requires login'''
 
[[Image:Equipment.jpg|500x500px|thumb|The Micro transfer printer is placed in F-4]]
 
[[Image:MTP image.jpg|1000px|thumb|left|Steps involved in pick and print]]
 
<br clear="all" />
 
==Equipment performance and process related parameters==
 
{|border="1" cellspacing="1" cellpadding="10" style="text-align:left;"
 
!style="background:silver; color:black;" width="60"|Purpose
|style="background:WhiteSmoke; color:black" colspan="2"|
Pick and Print


=Stylus Profiler: Dektak150=
|-
!style="background:silver; color:black;" width="60"|Material handling configuration
|style="background:WhiteSmoke; color:black" colspan="2"|
Manual


[[Image:DUV_wafers.jpg|500px|frameless|right|]]
|-
!style="background:silver; color:black;" width="60"|Stage max. travel time (X x Y mm)
|style="background:WhiteSmoke; color:black" colspan="2"|
300 x 300


TextTextTextTextTextText
|-
TextTextText
!style="background:silver; color:black;" width="60" |Source size (mm)
|style="background:WhiteSmoke; color:black" colspan="2"|
upto 150


TextTextTextTextText
|-
TextTextText
!style="background:silver; color:black;" width="60"|Target size (mm)
|style="background:WhiteSmoke; color:black" colspan="2"|
upto 150


|-
!style="background:silver; color:black;" width="60"|Alignment accuracy (single post stamp)
|style="background:WhiteSmoke; color:black" colspan="2"|
<0.5um


'''The user manual, technical information and contact information can be found in LabManager:'''
|-
[http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=457  Stylus profiler:Dektak150 in LabManager]
!style="background:silver; color:black" align="left" rowspan="3"|Allowed material
|style="background:WhiteSmoke; color:black" colspan="2"|
All cleanroom materials


TextTextTextTextTextText
TextText
|-
|}


==Equipment performance and process related parameters==
<br clear="all" />

Latest revision as of 12:46, 8 September 2023

The content on this page, including all images and pictures, was created by DTU Nanolab staff, unless otherwise stated.

Feedback to this page: click here


Micro Transfer Printer

Micro transfer printing is an emerging technique to transfer diverse and non-native components from source substrate to target substrate. Micro transfer printing is best for achieving heterogeneous integration, where micro-components from different sources are picked up by polymer stamp and precisely assembled onto different target substrate such as glass, plastic, ceramic and silicon. This method is known for increasing functionality and improving efficiency.

Micro transfer printer 1003 from Xdisplay was installed in year 2022 and placed in cleanroom F-4.

Equipment info in Lab Manager - requires login

The Micro transfer printer is placed in F-4
Steps involved in pick and print


Equipment performance and process related parameters

Purpose

Pick and Print

Material handling configuration

Manual

Stage max. travel time (X x Y mm)

300 x 300

Source size (mm)

upto 150

Target size (mm)

upto 150

Alignment accuracy (single post stamp)

<0.5um

Allowed material

All cleanroom materials