Created page with "'''Procedure of ultra-sectionning in images:''' 400px|left|thumb|1. Trimming resin block using Trim diamond knife<br /> [[File:8 (2).jpg|400px|left|thumb|2. Ul..." |
mNo edit summary |
||
| (6 intermediate revisions by 2 users not shown) | |||
| Line 1: | Line 1: | ||
'''Procedure of ultra-sectionning | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/LabAdviser/314/Preparation_314-307/Soft-matter/Ultramicrotomy click here]''' | ||
(''content by Marie Karen Tracy Hong Lin @DTU Nanolab, 2020'') | |||
[[Category:314]] | |||
[[Category:314-Preparation]] | |||
=Procedure of ultra-sectionning= | |||
== Step 1: Trimming resin block == | |||
[[File:1.jpg|400px|left|thumb|1. Trimming resin block using Trim diamond knife]]<br /> | [[File:1.jpg|400px|left|thumb|1. Trimming resin block using Trim diamond knife]]<br /> | ||
[[File:8 (2).jpg|400px|left|thumb| | <br clear="all" /> | ||
== Step 2: Mount sample to the ultramicrotome == | |||
<br clear="all" /> | |||
== Step 3: Mount glass or diamound knife to knife holder == | |||
<br clear="all" /> | |||
== Step 4: Ultra-sectioning of sample == | |||
[[File:8 (2).jpg|400px|left|thumb|4. Ultra-sectionning of sample using diamond knife with water boat]]<br /> | |||
<br clear="all" /> | |||
== Step 5: Fishing sections == | |||
[[File:9 (2).jpg|400px|left|thumb|5. Collecting sections using a Perfect loop]]<br /> | |||
<br clear="all" /> | |||
[[File:5 (2).jpg|400px|left|thumb| | == Step 6: Transfering sections to EM grid == | ||
[[File:5 (2).jpg|400px|left|thumb|6. Transfering sections on a grid]]<br /> | |||
Latest revision as of 11:12, 17 July 2023
Feedback to this page: click here (content by Marie Karen Tracy Hong Lin @DTU Nanolab, 2020)
Procedure of ultra-sectionning
Step 1: Trimming resin block

Step 2: Mount sample to the ultramicrotome
Step 3: Mount glass or diamound knife to knife holder
Step 4: Ultra-sectioning of sample

Step 5: Fishing sections

Step 6: Transfering sections to EM grid