Descum Comparison Table
| Plasma Asher 3: Descum | Plasma Asher 4 (Clean) | Plasma Asher 5 (Dirty) | |
|---|---|---|---|
| Purpose | Resist descum |
|
|
| Method | Plasma ashing | Plasma ashing | Plasma ashing |
| Process gasses | O2 (50 sccm) |
|
|
| Process power | 10-100 W (10-100%) | 150-1000 W | 150-1000 W |
| Substrate batch |
|
|
|
| Substrate materials |
|
|
|