| Front Image
|
-
|
|
|
<--Dry your sample -->
|
| <--Thermal treatment of your sample -->
|
Make a mask on your sample
|
|
|
| Clean your sample
|
| Entry page in LabAdviser
|
Techniques
|
Materials
|
| Wafer cleaning
|
Soap Sonic
|
Removes dust and particles
|
| 7-up & Piranha
|
Removes traces of organics and alkali ions
|
| RCA
|
Two step process to remove traces of organics and metals
|
| 5% HF
|
Removes native oxide
|
| IMEC
|
Removing dust, traces of organics and alkali ions and slightly polish the surface.
Make the surface hydrophillic
|
| Dry your sample Dry your sample
|
| Entry page in LabAdviser
|
Techniques
|
Materials
|
| Wafer and sample drying
|
Spin dryers
|
Whole wafers
|
| Critial point dryer
|
Sensitive wafers
|
| Ethanol fume drying
|
Sensitive wafers
|
| N2 blow drying
|
N2 pistols
|
| Thermal treatment of your sample Thermal treatment of your sample
|
| Entry page in LabAdviser
|
Techniques
|
Materials
|
| Thermal Process
|
Annealing (>350C)
|
Si, PECVD layers, Al, BCB curing, Polymer
|
| Oxidation
|
Si wafers
|
| Doping with B/P
|
Si wafers
|
| Pyrolysis
|
Resists: AZ, SU8, PDMS
|
| Rapid Thermal Anneal (RTP)
|
SiO2, Si3N4, Ti, III-V
|
|
Lithography/Baking
|
Baking (<300dg)
|
baking resist and polymers
|
| Make a mask on your sample Make a mask on your sample
|
| Entry page in LabAdviser
|
Techniques
|
Materials
|
| Lithography
|
Pattern design & Mask fabrication
|
|
| Photolithography
|
UV resists
|
| Deep UV lithography
|
DUV resists
|
| E-beam lithography
|
E-beam resists
|
| Imprinting
|
Polymers
|
|