Alcatel - A system for deposition of metals

 
positioned in cleanroom A-1.



The user manual, quality control procedure and results, user APV, technical information and contact information can be found in LabManager:

Alcatel in LabManager


Process information

Materials for e-beam evaporation


Equipment performance and process related parameters Alcatel

Purpose Deposition of metals and silicon
  • E-beam evaporation of metals
  • Sputtering of Silicon
Performance Film thickness
  • 10Å - 1µm* (for some materials)
Deposition rate
  • 2Å/s - 15Å/s
Process parameter range Process Temperature
  • Approximately room temperature
Process pressure
  • Low than 4*10-6 mbar
Substrates Batch size
  • One 4" wafer per run
  • Or several smaller pieces
  • Deposition on one side of the substrate
Substrate material allowed
  • Silicon wafers
  • Quartz wafers
  • Pyrex wafers
Material allowed on the substrate
  • Silicon oxide
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • Metals

* For thicknesses above 200 nm permission is requested.