Etching of Aluminium
Etching of aluminium can be done either by wet etch, dry etch or by sputtering with ions.
Comparison of Aluminium Etch Methods
|
|
Al wet etch 1
|
Al wet etch 2
|
Developer TMAH manual
|
ICP metal
|
IBE (Ionfab300+)
|
| Generel description
|
Wet etch of pure Al
|
Wet etch of Al + 1.5% Si
|
Wet etch/removal: TMAH
Mainly used for removing Al on e-beam resist after e-beam exposure, see process flow here
|
Dry plasma etch of Al
|
Sputtering of Al - pure physical etch
|
| Etch rate range
|
|
|
|
- ~350 nm/min (depending on features size and etch load)
|
- ~30nm/min (not tested yet)
|
| Etch profile
|
|
|
|
- Anisotropic (vertical sidewalls)
|
- Anisotropic (angles sidewalls, typical around 70 dg)
|
| Substrate size
|
|
|
|
- smaller pieces on a carrier wafer
- #1 100mm wafers (when set up to 100mm wafers)
- #1 150mm wafers (when set up to 150mm wafers)
|
Smaller pieces glued to carrier wafer
- #1 50mm wafer
- #1 100mm wafer
- #1 150mm wafer
- #1 200mm wafer
|
| Allowed materials
|
- Aluminium
- Silicon
- Silicon Oxide
- Silicon Nitride
- Silicon Oxynitride
- Photoresist
- E-beam resist
|
- Aluminium
- Silicon
- Silicon Oxide
- Silicon Nitride
- Silicon Oxynitride
- Photoresist
- E-beam resist
|
- Every thing that is allowed in the Developer: TMAH Manual
|
- Silicon
- Quartz/fused silica
- Photoresist/e-beam resist
- PolySilicon,
- Silicon oxide
- Silicon (oxy)nitride
- Aluminium
- Titanium
- Chromium
|
- Silicon
- Silicon oxides
- Silicon nitrides
- Metals from the +list
- Metals from the -list
- Alloys from the above list
- Stainless steel
- Glass
- III-V materials
- Resists
- Polymers
- Capton tape
|