Revision as of 12:02, 15 September 2026 by Meenadh (talk | contribs) (Created page with "==Spin Coater: LabSpin 04== 400px|thumb|Spin coater: LabSpin 04 is located in PolyFabLab in building 347 Spin Coater: LabSpin 04 is a model LabSpin6 TT spin coater from SUSS. It's primary purpose is spin coating of SU-8 resist. It was installed in PolyFabLab in 2025. The user manual, user APV, and contact information can be found in [http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=547 LabManager] - '''requires login''' '''Tr...")
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Spin Coater: LabSpin 04

Spin coater: LabSpin 04 is located in PolyFabLab in building 347

Spin Coater: LabSpin 04 is a model LabSpin6 TT spin coater from SUSS. It's primary purpose is spin coating of SU-8 resist. It was installed in PolyFabLab in 2025.

The user manual, user APV, and contact information can be found in LabManager - requires login

Training video (same tool in Cleanroom 346): LabSpin02 + 03

Process information

Useful information about resist dispense can be found here.

Equipment performance and process related parameters

Purpose
  • Spin coating of epoxy based resists
    • SU-8 series
    • SU-8 3000 series
    • SU-8 XFT series
    • mr-DWL series
  • Spin coating of other resists
Resist
  • manual dispense
Performance Coating thickness
  • SU-8 resists: 0.1-200 µm

Coating thickness range is dependent on specific resist formulation

Process parameters Spin speed

100 - 8000 rpm

Spin acceleration

200 - 4000 rpm/s (wrongly labelled 1/s^2 in the software)

Substrates Substrate size
  • chips, 5mm and up
  • 100 mm wafers
  • 150 mm wafers
Allowed materials

All PolyFabLab materials
See Cross Contamination Sheet in LabManager

Batch

1