Jump to content

Specific Process Knowledge/Lithography/Strip/wetBench06and07

From LabAdviser
Revision as of 12:20, 12 January 2026 by Jehem (talk | contribs) (Created page with "=Overview of wet bench 06 and 07= {| class="wikitable" |- ! !! Resist Strip !! Lift-off |- ! scope=row style="text-align: left;" | Process | Wet resist strip || Metal lift-off process |- ! scope=row style="text-align: left;" | Chemical | Remover 1165 (NMP) || Remover 1165 (NMP) |- ! scope=row style="text-align: left;" | Process tempera...")
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)

Overview of wet bench 06 and 07

Resist Strip Lift-off
Process Wet resist strip Metal lift-off process
Chemical Remover 1165 (NMP) Remover 1165 (NMP)
Process temperature Up to 65°C Up to 65°C
Substrate batch 1-25 wafers 1-25 wafers
Substrate size
  • 100 mm wafers
  • 150 mm wafers
  • 100 mm wafers
  • 150 mm wafers
Materials allowed
  • Silicon
  • Silicon oxide
  • Silicon nitride
  • Silicon oxynitride
All metals except Type IV (Pb, Te)