The current configuration is

{{Template:Peg2configcontent1
Currently valid from November 2020 onwards
Item The currently applied modification Comments
ItemName= Available gasses and gas chemistry ItemConfiguration=
  • SF6: 50 sccm
  • O2: 50 sccm
  • Ar: 283 sccm
  • N2: 500 sccm
  • He: 11 sccm
  • CO2: (It is not in the software)
ItemComment=OnlySF6 and O2 are used for Si, PR, and Cr etch. The rest is only make-up