Jump to content

Specific Process Knowledge/Characterization/Thickness Measurer

From LabAdviser

THIS PAGE IS UNDER CONSTRUCTION

Feedback to this page: click here

Thickness measurer

File:??.jpg
Thickness meassurer. Positioned in cleanroom 4

The purpose is to measure the thickness of wafers, depths of larger grooves or height of larger mesas.

Doing a KOH etch can it be helpful to insure no over etching by making a thickness measurement doing the etch.

The user manual, technical information and contact information can be found in LabManager:

Thickness measurer


Quality Control - Recipe Parameters and Limits

Quality Control (QC) for the Thickness measurer

The measured standard thickness is 0.1 mm. The measured result have to be within +- 0.005 mm. The QC is preformed ones a year.

Equipment performance and process related parameters

Purpose

Thickness measurer

  • Wafer
  • Depths of larger grooves
  • Heigth of larger mesas

Performance

Thickness within

0.5 µm

Process parameter range

Process Temperature

  • Room temperature
Process pressure
  • 1 atm

Substrates

Batch size

  • One sample per measure
Substrate materials allowed

No restriction.


Feedback to this page: click here


This is a micrometer-screw.

The Thickness measurer in Cleanroom 3

It measures with an accurracy within a few µm. The range is from a few µm up to 5mm. Measure the wafer in the box next to the meter. If this is ok, then other wafers can be measured. There is a calibration device by the DEKTAK. It is calibrated at 750µm.